{"title":"PREPARATION OF NEW POLYETHERPHTHALIMIDES BASED ON CHLORAL DERIVATIVES USING NUCLEOPHILIC POLYNITRO SUBSTITUTION REACTIONS","authors":"Abdullakh B. Ittiev, R. Kumykov","doi":"10.6060/ivkkt.20186201.5767","DOIUrl":null,"url":null,"abstract":"Non-previously described new bis (3-nitropthalimide) arylenes activated with two carbonyls and containing flexible “bridging” groups, in particular dichloroethylene and ketones between the phthalimide fragments of the dinitrocompounds were obtained. The reactivity of the dinitrophthalimides used is determined, first of all, by the position of (3 or 4) nitro groups, and not by the nature of the Ar residue; monomers containing nitro groups in position 3 are more reactive than systems containing nitro groups in position 4. The interaction of synthesized bis (nitropthalimide) arylenes containing central dichloroethylene and ketone groups between phthalimide fragments and bis-phenolate derivatives of chloral was carried out. Synthesis of polyetherphthalimides using the process of polynitro substitution was carried out under modified conditions with complete absence of moisture. In general, the reactions of polynitro substitution proceed rapidly under relatively mild conditions; when dipolar aprotic solvents or a mixture of them with toluene are used, relatively high molecular weight polymers are formed. It has been established that the rate of dissolution of monomers is an important factor affecting the reaction rate; this determines the possibility of the formation of relatively high-molecular polymers, even with some deviation from the equimolarity of the monomers. As the general conditions for the synthesis of polyetherphthalimides based on synthesized bis (3-nitropthalimide) arylenes and bis-phenols, the optimal conditions were: reaction temperature -60 °C, reaction time -1 h with equimolar monomer ratio and concentration of each of them 0.25 mol/l. The influence of moisture on the synthesis of polyetherimides using the reaction of nucleophilic polynitro substitution was studied. It is shown that the process in the maximally dry system in the DMSO medium or (DMSO / toluene) leads to the formation of polymers with hr at least 0.63 dl/g. All the polymers obtained are readily soluble in dipolar and aprotic solvents. The structure of all the obtained intermediates and monomers was confirmed by elemental analysis and IR spectroscopy. An analysis of the primary thermal characteristics of the polymers obtained showed that they are characterized by relatively high and near destruction temperatures was found that the largest oxygen index (CI) in polymers, where more macromolecules contain more dichloroethylene fragments, and the lowest CI in polymers with a high oxygen content. It is shown that the polymers obtained have satisfactory deformation-strength characteristics. A feature of synthesized polyetherphthalimides is a significant difference between the temperatures of intensive destruction and softening temperatures, which determines the possibility of their processing into products by injection molding. \n ","PeriodicalId":45993,"journal":{"name":"Izvestiya Vysshikh Uchebnykh Zavedenii Khimiya i Khimicheskaya Tekhnologiya","volume":null,"pages":null},"PeriodicalIF":0.6000,"publicationDate":"2018-12-30","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"1","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Izvestiya Vysshikh Uchebnykh Zavedenii Khimiya i Khimicheskaya Tekhnologiya","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.6060/ivkkt.20186201.5767","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"CHEMISTRY, MULTIDISCIPLINARY","Score":null,"Total":0}
引用次数: 1
Abstract
Non-previously described new bis (3-nitropthalimide) arylenes activated with two carbonyls and containing flexible “bridging” groups, in particular dichloroethylene and ketones between the phthalimide fragments of the dinitrocompounds were obtained. The reactivity of the dinitrophthalimides used is determined, first of all, by the position of (3 or 4) nitro groups, and not by the nature of the Ar residue; monomers containing nitro groups in position 3 are more reactive than systems containing nitro groups in position 4. The interaction of synthesized bis (nitropthalimide) arylenes containing central dichloroethylene and ketone groups between phthalimide fragments and bis-phenolate derivatives of chloral was carried out. Synthesis of polyetherphthalimides using the process of polynitro substitution was carried out under modified conditions with complete absence of moisture. In general, the reactions of polynitro substitution proceed rapidly under relatively mild conditions; when dipolar aprotic solvents or a mixture of them with toluene are used, relatively high molecular weight polymers are formed. It has been established that the rate of dissolution of monomers is an important factor affecting the reaction rate; this determines the possibility of the formation of relatively high-molecular polymers, even with some deviation from the equimolarity of the monomers. As the general conditions for the synthesis of polyetherphthalimides based on synthesized bis (3-nitropthalimide) arylenes and bis-phenols, the optimal conditions were: reaction temperature -60 °C, reaction time -1 h with equimolar monomer ratio and concentration of each of them 0.25 mol/l. The influence of moisture on the synthesis of polyetherimides using the reaction of nucleophilic polynitro substitution was studied. It is shown that the process in the maximally dry system in the DMSO medium or (DMSO / toluene) leads to the formation of polymers with hr at least 0.63 dl/g. All the polymers obtained are readily soluble in dipolar and aprotic solvents. The structure of all the obtained intermediates and monomers was confirmed by elemental analysis and IR spectroscopy. An analysis of the primary thermal characteristics of the polymers obtained showed that they are characterized by relatively high and near destruction temperatures was found that the largest oxygen index (CI) in polymers, where more macromolecules contain more dichloroethylene fragments, and the lowest CI in polymers with a high oxygen content. It is shown that the polymers obtained have satisfactory deformation-strength characteristics. A feature of synthesized polyetherphthalimides is a significant difference between the temperatures of intensive destruction and softening temperatures, which determines the possibility of their processing into products by injection molding.