{"title":"Effect of Cr 3 C 2 and VC on the Mechanical and Structural Properties of Sintered WC-10wt%Co Nano Powders","authors":"M. Mahmoodan, H. Aliakbarzadeh, F. Shahri","doi":"10.4236/WJNSE.2013.32005","DOIUrl":null,"url":null,"abstract":"The effect of addition of metallic carbides Cr3C2 and Cr3C2 + VC on structure and mechanical properties of WC-10 wt% Co nanocomposites have been studied. After preparing and compacting of the powders under pressure of 200 MPa, the samples were sintered at temperatures of 1370°C, 1410°C and 1450°C for 1 hour. Microstructural examinations by SEM show that the average grain size obtained for Cr3C2 + VC added alloys reduced 50 percent and also grain size distribution was narrower compared to those samples without grain growth inhibitors. Furthermore, co-addition of Cr3C2 and VC rise to a higher Vickers hardness and fracture toughness of the sintered alloys at 1410°C.","PeriodicalId":66816,"journal":{"name":"纳米科学与工程(英文)","volume":"3 1","pages":"35-39"},"PeriodicalIF":0.0000,"publicationDate":"2013-06-18","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"10","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"纳米科学与工程(英文)","FirstCategoryId":"1089","ListUrlMain":"https://doi.org/10.4236/WJNSE.2013.32005","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 10
Abstract
The effect of addition of metallic carbides Cr3C2 and Cr3C2 + VC on structure and mechanical properties of WC-10 wt% Co nanocomposites have been studied. After preparing and compacting of the powders under pressure of 200 MPa, the samples were sintered at temperatures of 1370°C, 1410°C and 1450°C for 1 hour. Microstructural examinations by SEM show that the average grain size obtained for Cr3C2 + VC added alloys reduced 50 percent and also grain size distribution was narrower compared to those samples without grain growth inhibitors. Furthermore, co-addition of Cr3C2 and VC rise to a higher Vickers hardness and fracture toughness of the sintered alloys at 1410°C.