{"title":"The effect of nanoparticle content and size on the morphology and crystallization behavior of poly(lactic acid)/silica nanocomposites","authors":"P. Saiprasit","doi":"10.3139/o999.01052019","DOIUrl":null,"url":null,"abstract":"Poly(lactic acid) (PLA)/silica nanocomposites with different filler loading and two different primary particle size of the filler were prepared by using a twin-screw extruder followed by injection molding. Morphological investigations showed, depending on the filler size and filler content, good dispersion with average agglomerate sizes of 38-60 nm. The spherulite growth and crystallization behavior of the nanocomposites discovers that smaller particles and a low filler loading leads to the fastest crystallization. The behavior can be explained by the fact that the small agglomerates and individual particles, visible in a standard Scanning Electron Microscope (SEM) are most frequently in this case. These particles serve as heterogeneous nucleation agents finally resulting in a fast crystallization of the PLA nanocomposite.","PeriodicalId":53661,"journal":{"name":"Zeitschrift Kunststofftechnik/Journal of Plastics Technology","volume":"1 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2019-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Zeitschrift Kunststofftechnik/Journal of Plastics Technology","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.3139/o999.01052019","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"Materials Science","Score":null,"Total":0}
引用次数: 0
Abstract
Poly(lactic acid) (PLA)/silica nanocomposites with different filler loading and two different primary particle size of the filler were prepared by using a twin-screw extruder followed by injection molding. Morphological investigations showed, depending on the filler size and filler content, good dispersion with average agglomerate sizes of 38-60 nm. The spherulite growth and crystallization behavior of the nanocomposites discovers that smaller particles and a low filler loading leads to the fastest crystallization. The behavior can be explained by the fact that the small agglomerates and individual particles, visible in a standard Scanning Electron Microscope (SEM) are most frequently in this case. These particles serve as heterogeneous nucleation agents finally resulting in a fast crystallization of the PLA nanocomposite.