{"title":"Soft Magnetic Properties of Electrodeposited CoNiFe Films","authors":"O. Shinoura;A. Kamijima;Y. Narumiya","doi":"10.1109/TJMJ.1994.4565934","DOIUrl":null,"url":null,"abstract":"The soft magnetic properties of electrodeposited CoNiFe films were studied. Films composed of 30 to 50 wt% Co, 23 to 35 wt% Ni and 25 to 35 wt% Fe alloy with a high saturation flux density of more than 1.5 T exhibit low coercivities under 0.2 Oe. Film composed of 40 Co-30 Ni-30 Fe alloy, consisting primarily of an fcc phase with some bec phase material and created by annealing at 300°C, has excellent soft magnetic properties (H\n<sub>c</sub>\n=0.06 Oe, μ=3200, B\n<inf>s</inf>\n=1.8 T). This bcc phase makes an appearance during the first stage of crystallization at 287°C. The structure is thermally unstable, and is due to a special feature of electrodeposition. During the annealing, H\n<sub>2</sub>\nO, H\n<sub>2</sub>\n and CO\n<sub>2</sub>\n were released from the film, but the patterns of generation of these gases bear little relation to the DSC pattern.","PeriodicalId":100647,"journal":{"name":"IEEE Translation Journal on Magnetics in Japan","volume":"9 5","pages":"118-123"},"PeriodicalIF":0.0000,"publicationDate":"1994-09-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://sci-hub-pdf.com/10.1109/TJMJ.1994.4565934","citationCount":"18","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"IEEE Translation Journal on Magnetics in Japan","FirstCategoryId":"1085","ListUrlMain":"https://ieeexplore.ieee.org/document/4565934/","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 18
Abstract
The soft magnetic properties of electrodeposited CoNiFe films were studied. Films composed of 30 to 50 wt% Co, 23 to 35 wt% Ni and 25 to 35 wt% Fe alloy with a high saturation flux density of more than 1.5 T exhibit low coercivities under 0.2 Oe. Film composed of 40 Co-30 Ni-30 Fe alloy, consisting primarily of an fcc phase with some bec phase material and created by annealing at 300°C, has excellent soft magnetic properties (H
c
=0.06 Oe, μ=3200, B
s
=1.8 T). This bcc phase makes an appearance during the first stage of crystallization at 287°C. The structure is thermally unstable, and is due to a special feature of electrodeposition. During the annealing, H
2
O, H
2
and CO
2
were released from the film, but the patterns of generation of these gases bear little relation to the DSC pattern.