{"title":"Manufacture, Characterization, and Structure Analysis of Melt-Spun Fibers Derived from Paramylon Esters","authors":"Hongyi Gan, T. Kabe, T. Iwata","doi":"10.2115/fiberst.2020-0018","DOIUrl":null,"url":null,"abstract":": Paramylon̶a β -1,3-glucan photoproduced by Euglena ̶is a promising raw material for bio-based plastics. Three kinds of paramylon ester derivatives̶paramylon propionate (PaPr), paramylon butyrate (PaBu), and paramylon valerate (PaVa)̶were synthesized to manufacture melt-spun fibers. The melt processing temperatures were determined by combining differential scanning calorimetry (DSC) and a melt flow test. The molecular orientation, crystallinity, and tensile properties of the melt-spun fibers were investigated using a polarized optical microscope (POM), wide-angle X-ray diffraction (WAXD), and tensile testing, respectively. The POM revealed that the PaPr molecular chains were aligned along the spinning direction, despite variation in the take-up rate. However, WAXD confirmed that crystallization only occurred in PaPr fibers spun at a higher take-up rate of over 108 m/min, suggesting that crystallization is induced by high shearing force. This phenomenon seems to be due to the rigid mainchain structure consisting of pyranose rings. With further annealing of the PaPr fibers, the tensile strength increased with an increase in crystallinity. These tendencies were also observed in the PaBu and PaVa melt-spun fibers. The melt-spun fibers of paramylon ester derivatives were manufactured from powders without any additives.","PeriodicalId":54299,"journal":{"name":"Journal of Fiber Science and Technology","volume":null,"pages":null},"PeriodicalIF":0.3000,"publicationDate":"2020-05-30","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"6","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Fiber Science and Technology","FirstCategoryId":"88","ListUrlMain":"https://doi.org/10.2115/fiberst.2020-0018","RegionNum":4,"RegionCategory":"工程技术","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"MATERIALS SCIENCE, TEXTILES","Score":null,"Total":0}
引用次数: 6

Abstract

: Paramylon̶a β -1,3-glucan photoproduced by Euglena ̶is a promising raw material for bio-based plastics. Three kinds of paramylon ester derivatives̶paramylon propionate (PaPr), paramylon butyrate (PaBu), and paramylon valerate (PaVa)̶were synthesized to manufacture melt-spun fibers. The melt processing temperatures were determined by combining differential scanning calorimetry (DSC) and a melt flow test. The molecular orientation, crystallinity, and tensile properties of the melt-spun fibers were investigated using a polarized optical microscope (POM), wide-angle X-ray diffraction (WAXD), and tensile testing, respectively. The POM revealed that the PaPr molecular chains were aligned along the spinning direction, despite variation in the take-up rate. However, WAXD confirmed that crystallization only occurred in PaPr fibers spun at a higher take-up rate of over 108 m/min, suggesting that crystallization is induced by high shearing force. This phenomenon seems to be due to the rigid mainchain structure consisting of pyranose rings. With further annealing of the PaPr fibers, the tensile strength increased with an increase in crystallinity. These tendencies were also observed in the PaBu and PaVa melt-spun fibers. The melt-spun fibers of paramylon ester derivatives were manufactured from powders without any additives.
以paramam酰胺酯为原料的熔融纺丝纤维的制造、表征和结构分析
:由绿藻光产生的Paramylon - a β -1,3-葡聚糖是一种很有前途的生物基塑料原料。合成了三种酰胺酯衍生物——丙酸酰胺(PaPr)、丁酸酰胺(pab)和戊酸酰胺(PaVa)——用于制备熔融纺丝纤维。采用差示扫描量热法(DSC)和熔体流动试验相结合的方法确定了熔体加工温度。利用偏光显微镜(POM)、广角x射线衍射(WAXD)和拉伸测试分别研究了熔融纺丝纤维的分子取向、结晶度和拉伸性能。POM显示,尽管吸收率不同,但PaPr分子链沿自旋方向排列。然而,WAXD证实,结晶只发生在吸收率高于108 m/min的PaPr纤维中,这表明结晶是由高剪切力引起的。这种现象似乎是由于由吡喃糖环组成的刚性主链结构所致。进一步退火后,纤维的抗拉强度随着结晶度的增加而增加。在PaBu和PaVa熔纺纤维中也观察到这些趋势。以不添加任何添加剂的粉末为原料制备了酰胺酯衍生物的熔融纺丝纤维。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
Journal of Fiber Science and Technology
Journal of Fiber Science and Technology Materials Science-Materials Science (miscellaneous)
CiteScore
0.50
自引率
0.00%
发文量
17
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信