{"title":"Structural behavior of reinforced concrete incorporating glass waste as coarse aggregate","authors":"S. M. Hama, Z. M. Ali, H. Zayan, A. Mahmoud","doi":"10.1080/24705314.2023.2165470","DOIUrl":null,"url":null,"abstract":"ABSTRACT Most of the previous work related to using waste glass as aggregate in concrete focused on mechanical properties, so this investigation focused on the structural behavior of reinforced concrete (RC) beams incorporating waste glass as a partial replacement of aggregate. This research investigated the influence of waste glass as a replacement for coarse aggregate in the following percentages: 0% (reference), 25% and 50%, on the structural behavior of RC beams. This work uses six beams (cross-section 150 × 150 mm and span length of 900 mm). In addition to the effect of glass aggregate content on structural behavior, another parameter was considered, which is the effect of longitudinal steel reinforcement ratio (2Ø10 mm, ρ = 0.0083; 2Ø16 mm, ρ = 0.0222). The beams containing waste glass aggregate (WGA) showed a more ductile behavior and were less stiff compared to reference beams. Beams containing WGA showed good strength and satisfactory structural performance compared with the reference beam.","PeriodicalId":43844,"journal":{"name":"Journal of Structural Integrity and Maintenance","volume":"24 1","pages":"59 - 66"},"PeriodicalIF":3.0000,"publicationDate":"2023-01-02","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"3","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Structural Integrity and Maintenance","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1080/24705314.2023.2165470","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q2","JCRName":"ENGINEERING, CIVIL","Score":null,"Total":0}
引用次数: 3

Abstract

ABSTRACT Most of the previous work related to using waste glass as aggregate in concrete focused on mechanical properties, so this investigation focused on the structural behavior of reinforced concrete (RC) beams incorporating waste glass as a partial replacement of aggregate. This research investigated the influence of waste glass as a replacement for coarse aggregate in the following percentages: 0% (reference), 25% and 50%, on the structural behavior of RC beams. This work uses six beams (cross-section 150 × 150 mm and span length of 900 mm). In addition to the effect of glass aggregate content on structural behavior, another parameter was considered, which is the effect of longitudinal steel reinforcement ratio (2Ø10 mm, ρ = 0.0083; 2Ø16 mm, ρ = 0.0222). The beams containing waste glass aggregate (WGA) showed a more ductile behavior and were less stiff compared to reference beams. Beams containing WGA showed good strength and satisfactory structural performance compared with the reference beam.
含玻璃废料粗集料的钢筋混凝土结构性能
以前的大部分工作都是关于在混凝土中使用废玻璃作为骨料的力学性能,因此本研究的重点是使用废玻璃作为骨料部分替代品的钢筋混凝土(RC)梁的结构性能。本研究考察了废玻璃替代粗骨料的比例:0%(参考)、25%和50%对RC梁结构性能的影响。本工程采用6根梁(截面150 × 150毫米,跨度900毫米)。除了玻璃骨料含量对结构性能的影响外,还考虑了另一个参数,即纵向钢筋配筋率的影响(2Ø10 mm, ρ = 0.0083;2Ø16 mm, ρ = 0.0222)。含有废玻璃骨料(WGA)的梁与参考梁相比具有更强的延性和更小的刚度。与参考梁相比,含有WGA的梁具有良好的强度和令人满意的结构性能。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
CiteScore
3.90
自引率
9.50%
发文量
24
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信