Tensile Property of Al-Mg-Sc-Zr Alloy at Cryogenic Temperature

W. Zhao, D. Yan, Xiutao Li, L. Rong, Yuntao Li
{"title":"Tensile Property of Al-Mg-Sc-Zr Alloy at Cryogenic Temperature","authors":"W. Zhao, D. Yan, Xiutao Li, L. Rong, Yuntao Li","doi":"10.1063/1.2192348","DOIUrl":null,"url":null,"abstract":"The tensile property and fracture characteristic of Al‐Mg‐Sc‐Zr alloy have been investigated at 77 K, 123 K, 173 K, 223 K and 300 K respectively. Both the strength and elongation improved with decreasing temperature from 300 K to 77 K, particularly between 123 K and 77 K. However, the reduction of area exhibited a maximum at around 173 K. The fractographs of tensile specimens show a completely dimple‐type ductile mode of fracture at 77 K and mixed type of fracture at 300 K, and the primary Al3(Sc,Zr) and Al6(Mn,Fe) phases are responsible for void and crack initiation at their interface with the matrix at cryogenic temperature.","PeriodicalId":80359,"journal":{"name":"Advances in cryogenic engineering","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"2006-04-21","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://sci-hub-pdf.com/10.1063/1.2192348","citationCount":"1","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Advances in cryogenic engineering","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1063/1.2192348","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 1

Abstract

The tensile property and fracture characteristic of Al‐Mg‐Sc‐Zr alloy have been investigated at 77 K, 123 K, 173 K, 223 K and 300 K respectively. Both the strength and elongation improved with decreasing temperature from 300 K to 77 K, particularly between 123 K and 77 K. However, the reduction of area exhibited a maximum at around 173 K. The fractographs of tensile specimens show a completely dimple‐type ductile mode of fracture at 77 K and mixed type of fracture at 300 K, and the primary Al3(Sc,Zr) and Al6(Mn,Fe) phases are responsible for void and crack initiation at their interface with the matrix at cryogenic temperature.
Al-Mg-Sc-Zr合金的低温拉伸性能
研究了Al - Mg - Sc - Zr合金在77 K、123 K、173 K、223 K和300 K下的拉伸性能和断裂特征。从300 K到77 K,强度和伸长率随温度的降低而提高,特别是在123 K到77 K之间。而面积的减小在173 K左右达到最大值。拉伸试样的断口形貌在77 K时表现为完全韧窝型韧性断裂,在300 K时表现为混合型断裂,在低温下,Al3(Sc,Zr)和Al6(Mn,Fe)初生相在其与基体的界面处产生空洞和裂纹。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信