{"title":"KTIG–MIG hybrid arc welding process","authors":"QingPeng Xiu, Zuming Liu, Xingchuan Zhao","doi":"10.1080/13621718.2023.2213916","DOIUrl":null,"url":null,"abstract":"Metal-inert gas welding is an important welding process but the process instability easily induces spatter and undercut defects. To improve the welding process stability, a new hybrid arc welding process, named KTIG–MIG, was proposed in this paper. Arc characteristics were preliminarily studied. It is found that in KTIG–MIG hybrid welding, MIG arc is stable even it is shielded with pure argon gas; stable spray transfer is easily achieved in a much wider process window, especially the lowest voltage to achieve spray transfer is greatly reduced; KTIG arc voltage decreases than that in single KTIG arc, and MIG arc current is higher than the pre-set value. Cooling state of the KTIG tungsten plays a key role in slowing tungsten erosion.","PeriodicalId":21729,"journal":{"name":"Science and Technology of Welding and Joining","volume":"28 1","pages":"728 - 737"},"PeriodicalIF":2.9000,"publicationDate":"2023-05-18","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Science and Technology of Welding and Joining","FirstCategoryId":"88","ListUrlMain":"https://doi.org/10.1080/13621718.2023.2213916","RegionNum":3,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q2","JCRName":"MATERIALS SCIENCE, MULTIDISCIPLINARY","Score":null,"Total":0}
引用次数: 0
Abstract
Metal-inert gas welding is an important welding process but the process instability easily induces spatter and undercut defects. To improve the welding process stability, a new hybrid arc welding process, named KTIG–MIG, was proposed in this paper. Arc characteristics were preliminarily studied. It is found that in KTIG–MIG hybrid welding, MIG arc is stable even it is shielded with pure argon gas; stable spray transfer is easily achieved in a much wider process window, especially the lowest voltage to achieve spray transfer is greatly reduced; KTIG arc voltage decreases than that in single KTIG arc, and MIG arc current is higher than the pre-set value. Cooling state of the KTIG tungsten plays a key role in slowing tungsten erosion.
期刊介绍:
Science and Technology of Welding and Joining is an international peer-reviewed journal covering both the basic science and applied technology of welding and joining.
Its comprehensive scope encompasses all welding and joining techniques (brazing, soldering, mechanical joining, etc.) and aspects such as characterisation of heat sources, mathematical modelling of transport phenomena, weld pool solidification, phase transformations in weldments, microstructure-property relationships, welding processes, weld sensing, control and automation, neural network applications, and joining of advanced materials, including plastics and composites.