Pengaruh Suhu Sintering terhadap Pembentukan Senyawa Gd0,95La0,05Ba1,95Sr0,05Cu3O7-?

Asni Mulyati Jeni, Made Sumadiyasa, Ida Bagus Made Suryatika
{"title":"Pengaruh Suhu Sintering terhadap Pembentukan Senyawa Gd0,95La0,05Ba1,95Sr0,05Cu3O7-?","authors":"Asni Mulyati Jeni, Made Sumadiyasa, Ida Bagus Made Suryatika","doi":"10.24843/bf.2023.v24.i01.p02","DOIUrl":null,"url":null,"abstract":"Research has been conducted variations in sintering temperature between 900 ºC – 950 ºC for 12 hours on the synthesis phase of Gd1Ba2Cu3O7-d substituted La and Sr with stoichiometric composition Gd0,95La0,05Ba1,95Sr0,05Cu3O7-d. This study is intended to find out at what temperature the compound Gd0,95La0,05Ba1,95Sr0,05Cu3O7-d  can be formed to the maximum. Samples with composition Gd0,95La0,05Ba1,95Sr0,05Cu3O7-d made from the raw materials Gd2O3, La2O3, BaO, Sr2O3 and CuO. Samples are synthesized using solid-state reaction method by wet mixing with nitric acid (HNO3) as solvent. The sample is sintering in the form of pellets in the furnace without annealing of oxygen gas. The synthesis results were characterized by X-Ray Diffraction (XRD) and analyzed with the Match-3 Program. By using the Entry number 96-153-9606, the results of it analysis showed that sintering temperature had an impact on the formation of phase compounds Gd0,95La0,05Ba1,95Sr0,05Cu3O7-d. Show that the volume fraction is increases with increasing of the sintering temperature, especially from temperatures of 930 ºC to 950 ºC. The highest volume fraction of 75,4263 % was obtained in samples that sintering at 950 ºC. Refinement results with Rietveld analysis method showed phase Gd0,95La0,05Ba1,95Sr0,05Cu3O7-d formed is in orthorhombic symmetry. The volume of cell units is likely to increase as the temperature increases.","PeriodicalId":32375,"journal":{"name":"Buletin Fisika","volume":" ","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2021-09-21","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Buletin Fisika","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.24843/bf.2023.v24.i01.p02","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

Research has been conducted variations in sintering temperature between 900 ºC – 950 ºC for 12 hours on the synthesis phase of Gd1Ba2Cu3O7-d substituted La and Sr with stoichiometric composition Gd0,95La0,05Ba1,95Sr0,05Cu3O7-d. This study is intended to find out at what temperature the compound Gd0,95La0,05Ba1,95Sr0,05Cu3O7-d  can be formed to the maximum. Samples with composition Gd0,95La0,05Ba1,95Sr0,05Cu3O7-d made from the raw materials Gd2O3, La2O3, BaO, Sr2O3 and CuO. Samples are synthesized using solid-state reaction method by wet mixing with nitric acid (HNO3) as solvent. The sample is sintering in the form of pellets in the furnace without annealing of oxygen gas. The synthesis results were characterized by X-Ray Diffraction (XRD) and analyzed with the Match-3 Program. By using the Entry number 96-153-9606, the results of it analysis showed that sintering temperature had an impact on the formation of phase compounds Gd0,95La0,05Ba1,95Sr0,05Cu3O7-d. Show that the volume fraction is increases with increasing of the sintering temperature, especially from temperatures of 930 ºC to 950 ºC. The highest volume fraction of 75,4263 % was obtained in samples that sintering at 950 ºC. Refinement results with Rietveld analysis method showed phase Gd0,95La0,05Ba1,95Sr0,05Cu3O7-d formed is in orthorhombic symmetry. The volume of cell units is likely to increase as the temperature increases.
辐射的影响。。。
研究了900℃~ 950℃烧结12小时后,Gd1Ba2Cu3O7-d取代La和Sr合成相的化学计量成分为Gd0,95La0,05Ba1,95Sr0,05Cu3O7-d。本研究旨在找出在什么温度下能最大限度地形成化合物Gd0,95La0,05Ba1,95Sr0,05Cu3O7-d。以Gd2O3、La2O3、BaO、Sr2O3和CuO为原料制备了成分为Gd0、95La0、05Ba1、95Sr0、05Cu3O7-d的样品。采用固相反应法,以硝酸(HNO3)为溶剂,湿法混合合成样品。样品在没有氧气退火的情况下,以球团的形式在炉中烧结。用x射线衍射(XRD)对合成结果进行了表征,并用Match-3程序对合成结果进行了分析。采用进样号96-153-9606进行分析,结果表明,烧结温度对相化合物Gd0、95La0、05Ba1、95Sr0、05Cu3O7-d的形成有影响。结果表明:随着烧结温度的升高,烧结材料的体积分数呈增大趋势,烧结温度在930 ~ 950℃范围内尤为明显。在950℃烧结时,样品的体积分数最高,为75,4263 %。Rietveld法细化结果表明,相Gd0、95La0、05Ba1、95Sr0、05Cu3O7-d形成正交对称。随着温度的升高,电池单元的体积可能会增加。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
自引率
0.00%
发文量
0
审稿时长
24 weeks
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信