A. Hamisu, S. S. Bala, A. Bello, A. Abubakar, A. A. Adeyi
{"title":"Sol-gel template synthesis of visible photoactive Cu-S co-doped mesoporous TiO2 catalyst","authors":"A. Hamisu, S. S. Bala, A. Bello, A. Abubakar, A. A. Adeyi","doi":"10.1080/23249676.2022.2116116","DOIUrl":null,"url":null,"abstract":"A new visible photoactive catalyst (Cu, S/PEG-PVA/TiO2) was synthesized by the sol-gel method. In addition, Cu, S/TiO2 and Bare TiO2 were synthesized to compare their properties and activities. The synthesized catalysts were characterized using XRD, N2 adsorption–desorption measurements, SEM, TEM, EDX, UV-Vis spectroscopy and TGA. The photocatalytic activities of the synthesized photocatalysts were evaluated by measuring the photocatalytic degradation of 4-nitrophenol under visible light irradiation. Then, the impacts of three parameters, (catalyst loading, pH and H2O2 concentration) for optimization and modelization of the 4-nitrophenol photodegradation were studied using the response surface methodology. Optimal conditions obtained from statistical analysis at a catalyst loading of 1 gL−1, pH of 3.98 and H2O2 concentration of 8 mg/L have shown the highest 4-NP percentage degradation of 70.5% in 1 h. The results predicted by the models were found to be in good agreement with those obtained by performing the experiment (R 2 = 0.9443 and Adj-R 2 = 0.9038).","PeriodicalId":51911,"journal":{"name":"Journal of Applied Water Engineering and Research","volume":null,"pages":null},"PeriodicalIF":1.4000,"publicationDate":"2022-09-02","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Applied Water Engineering and Research","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1080/23249676.2022.2116116","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"WATER RESOURCES","Score":null,"Total":0}
引用次数: 0
Abstract
A new visible photoactive catalyst (Cu, S/PEG-PVA/TiO2) was synthesized by the sol-gel method. In addition, Cu, S/TiO2 and Bare TiO2 were synthesized to compare their properties and activities. The synthesized catalysts were characterized using XRD, N2 adsorption–desorption measurements, SEM, TEM, EDX, UV-Vis spectroscopy and TGA. The photocatalytic activities of the synthesized photocatalysts were evaluated by measuring the photocatalytic degradation of 4-nitrophenol under visible light irradiation. Then, the impacts of three parameters, (catalyst loading, pH and H2O2 concentration) for optimization and modelization of the 4-nitrophenol photodegradation were studied using the response surface methodology. Optimal conditions obtained from statistical analysis at a catalyst loading of 1 gL−1, pH of 3.98 and H2O2 concentration of 8 mg/L have shown the highest 4-NP percentage degradation of 70.5% in 1 h. The results predicted by the models were found to be in good agreement with those obtained by performing the experiment (R 2 = 0.9443 and Adj-R 2 = 0.9038).
期刊介绍:
JAWER’s paradigm-changing (online only) articles provide directly applicable solutions to water engineering problems within the whole hydrosphere (rivers, lakes groundwater, estuaries, coastal and marine waters) covering areas such as: integrated water resources management and catchment hydraulics hydraulic machinery and structures hydraulics applied to water supply, treatment and drainage systems (including outfalls) water quality, security and governance in an engineering context environmental monitoring maritime hydraulics ecohydraulics flood risk modelling and management water related hazards desalination and re-use.