{"title":"Deposition of titanium silicide on stainless steel AISI 304 surface","authors":"A. Burkov, V. Krutikova","doi":"10.17212/1994-6309-2022-24.4-127-137","DOIUrl":null,"url":null,"abstract":"Introduction. Metal-ceramic coatings based on titanium silicide are promising for protecting stainless steel AISI 304 from wear, corrosion and high-temperature oxidation. Purpose of the work: to investigate the stainless steel AISI 304 surface layer structure after electrospark deposition in a mixture of titanium granules with silicon powder, and to study oxidation resistance, corrosion resistance and tribotechnical properties of the obtained coatings. Research methodology. Fe-Ti-Si coatings on the stainless steel AISI 304 samples were obtained by electrospark machining with a non-localized electrode consisting of titanium granules and 2.6-6 vol.% mixture of titanium and crystalline silicon powders. Results and discussion: it is shown that a stable positive gain of the cathode is observed when the proportion of silicon in the powder mixture does not exceed 32 vol.%. The phase composition of the coatings includes: a solid solution of chromium in iron, titanium silicide Ti5Si3, titanium and silicon, which is confirmed by the energy dispersion analysis data. The microhardness of Fe-Ti-Si coatings ranges from 10.05 to 12.86 GPa, which is 5-6 times higher than that of uncoated steel AISI 304. The coefficient of friction of the coatings is about 20% lower compared to steel AISI 304 and hovers around 0.71-0.73. Wear tests in dry sliding mode show that Fe-Ti-Si coatings can increase the wear resistance of steel AISI 304 up to 6 times. The oxidation resistance of the coatings at a temperature of 900 ̊С is 7-12 times higher as compared to steel AISI 304. The conducted studies have shown that new electrospark Fe-Ti-Si coatings can increase corrosion resistance, oxidation resistance, microhardness, as well as reduce the coefficient of friction and wear rate of the stainless steel AISI 304 surface.","PeriodicalId":42889,"journal":{"name":"Obrabotka Metallov-Metal Working and Material Science","volume":" ","pages":""},"PeriodicalIF":0.4000,"publicationDate":"2022-12-15","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"1","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Obrabotka Metallov-Metal Working and Material Science","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.17212/1994-6309-2022-24.4-127-137","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"METALLURGY & METALLURGICAL ENGINEERING","Score":null,"Total":0}
引用次数: 1
Abstract
Introduction. Metal-ceramic coatings based on titanium silicide are promising for protecting stainless steel AISI 304 from wear, corrosion and high-temperature oxidation. Purpose of the work: to investigate the stainless steel AISI 304 surface layer structure after electrospark deposition in a mixture of titanium granules with silicon powder, and to study oxidation resistance, corrosion resistance and tribotechnical properties of the obtained coatings. Research methodology. Fe-Ti-Si coatings on the stainless steel AISI 304 samples were obtained by electrospark machining with a non-localized electrode consisting of titanium granules and 2.6-6 vol.% mixture of titanium and crystalline silicon powders. Results and discussion: it is shown that a stable positive gain of the cathode is observed when the proportion of silicon in the powder mixture does not exceed 32 vol.%. The phase composition of the coatings includes: a solid solution of chromium in iron, titanium silicide Ti5Si3, titanium and silicon, which is confirmed by the energy dispersion analysis data. The microhardness of Fe-Ti-Si coatings ranges from 10.05 to 12.86 GPa, which is 5-6 times higher than that of uncoated steel AISI 304. The coefficient of friction of the coatings is about 20% lower compared to steel AISI 304 and hovers around 0.71-0.73. Wear tests in dry sliding mode show that Fe-Ti-Si coatings can increase the wear resistance of steel AISI 304 up to 6 times. The oxidation resistance of the coatings at a temperature of 900 ̊С is 7-12 times higher as compared to steel AISI 304. The conducted studies have shown that new electrospark Fe-Ti-Si coatings can increase corrosion resistance, oxidation resistance, microhardness, as well as reduce the coefficient of friction and wear rate of the stainless steel AISI 304 surface.