{"title":"Effect of sintering temperatures on temperature coefficient of capacitance of KCa2Nb3O10 bulk-layered perovskite","authors":"Jeong-Yeon Kim, Gyo-Hee Hong, Se Yun Kim, Seong-Mee Hwang, W. Shin, W. Seo, Sang‐il Kim, Hyun-sik Kim","doi":"10.1080/21870764.2023.2228090","DOIUrl":null,"url":null,"abstract":"ABSTRACT Multilayer ceramic capacitors (MLCCs) for electric vehicles require their room temperature capacitance to change ≤ ±15% at −55°C to 200°C. The dielectric constant (ε) of BaTiO3, a dielectric material widely used in MLCCs, drops at >125°C making its application to electric vehicles difficult. Here, we propose KCa2Nb3O10 (KCNO)-layered perovskite as a strong candidate for electric vehicle MLCCs as its ε does not change abruptly with temperature. The effect of sintering temperature on the temperature coefficient of capacitance (TCC) of KCNO is studied. The KCNO powder calcined at 900–1200°C is sintered at 1200°C–1300°C. Microstructure and temperature-dependent ε are determined by the sintering temperature, while the sintered density is related to the difference between the calcining and sintering temperatures. Only the room temperature ε of the samples sintered at 1300°C (except the one calcined at 900°C) varies ≤ ±15% at 25°C–200°C (ε ~250 at room temperature). The sample calcined at 1100°C and sintered at 1300°C has highly elongated grains and the highest activation energy. These factors are responsible for the TCC of the 1300°C sintered KCNO being ≤ ±15% at 25–200°C.","PeriodicalId":15130,"journal":{"name":"Journal of Asian Ceramic Societies","volume":"11 1","pages":"395 - 405"},"PeriodicalIF":2.2000,"publicationDate":"2023-06-27","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Asian Ceramic Societies","FirstCategoryId":"88","ListUrlMain":"https://doi.org/10.1080/21870764.2023.2228090","RegionNum":4,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q2","JCRName":"MATERIALS SCIENCE, CERAMICS","Score":null,"Total":0}
引用次数: 0

Abstract

ABSTRACT Multilayer ceramic capacitors (MLCCs) for electric vehicles require their room temperature capacitance to change ≤ ±15% at −55°C to 200°C. The dielectric constant (ε) of BaTiO3, a dielectric material widely used in MLCCs, drops at >125°C making its application to electric vehicles difficult. Here, we propose KCa2Nb3O10 (KCNO)-layered perovskite as a strong candidate for electric vehicle MLCCs as its ε does not change abruptly with temperature. The effect of sintering temperature on the temperature coefficient of capacitance (TCC) of KCNO is studied. The KCNO powder calcined at 900–1200°C is sintered at 1200°C–1300°C. Microstructure and temperature-dependent ε are determined by the sintering temperature, while the sintered density is related to the difference between the calcining and sintering temperatures. Only the room temperature ε of the samples sintered at 1300°C (except the one calcined at 900°C) varies ≤ ±15% at 25°C–200°C (ε ~250 at room temperature). The sample calcined at 1100°C and sintered at 1300°C has highly elongated grains and the highest activation energy. These factors are responsible for the TCC of the 1300°C sintered KCNO being ≤ ±15% at 25–200°C.
烧结温度对KCa2Nb3O10块体层状钙钛矿电容温度系数的影响
摘要:电动汽车用多层陶瓷电容器(MLCC)要求其室温电容在−55°C至200°C时变化≤±15%。BaTiO3是一种广泛用于MLCC的介电材料,其介电常数(ε)在 >125°C,使其难以应用于电动汽车。在这里,我们提出KCa2Nb3O10(KCNO)层状钙钛矿作为电动汽车MLCC的有力候选者,因为其ε不会随温度突然变化。研究了烧结温度对KCNO电容温度系数的影响。在900–1200°C下煅烧的KCNO粉末在1200°C–1300°C下烧结。微观结构和温度相关的ε由烧结温度决定,而烧结密度与煅烧温度和烧结温度之间的差异有关。只有在1300°C下烧结的样品(在900°C下煅烧的样品除外)的室温ε在25°C–200°C下变化≤±15%(室温下ε~250)。在1100°C下煅烧并在1300°C下烧结的样品具有高度伸长的晶粒和最高的活化能。这些因素是1300°C烧结KCNO在25–200°C时TCC≤±15%的原因。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
Journal of Asian Ceramic Societies
Journal of Asian Ceramic Societies Materials Science-Ceramics and Composites
CiteScore
5.00
自引率
4.30%
发文量
78
审稿时长
10 weeks
期刊介绍: The Journal of Asian Ceramic Societies is an open access journal publishing papers documenting original research and reviews covering all aspects of science and technology of Ceramics, Glasses, Composites, and related materials. These papers include experimental and theoretical aspects emphasizing basic science, processing, microstructure, characteristics, and functionality of ceramic materials. The journal publishes high quality full papers, letters for rapid publication, and in-depth review articles. All papers are subjected to a fair peer-review process.
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信