SYHNTHESIS OF CHITOSAN MODIFIED POLYURETHANE FOAM FOR ADSOPRTION OF MERCURY (II) IONS

D. Darmadi, M. Irfan, M Iqhramullah, M. Marlina, M. R. Lubis
{"title":"SYHNTHESIS OF CHITOSAN MODIFIED POLYURETHANE FOAM FOR ADSOPRTION OF MERCURY (II) IONS","authors":"D. Darmadi, M. Irfan, M Iqhramullah, M. Marlina, M. R. Lubis","doi":"10.15294/JBAT.V7I1.13614","DOIUrl":null,"url":null,"abstract":"Mercury from the traditional gold mining activities in Aceh Jaya Regency causes water source and thus residents are exposed to mercury metals. In organic and inorganic conditions, mercury is toxic to the human body, causes damage to the nerve system, kidney failure, heart failure, blood pressure disorders, and damage to the immune system. The problem of mercury contamination can be chemically solved in various ways. This research uses polyurethane foam to adsorb mercury from water. The adsorption and selectivity of polyurethane foam adsorption can be improved through modification with Chitosan. In this research, preheating temperature, glycerol and toluene di-isocyanate (TDI) compositions greatly affect the physical form of foam. The condition under which optimal glycerol composition used for synthesizing the polyurethane foams is 20% (w/w of mixture A). This glycerol composition results in polyurethane foams with an optimum ratio of the mixture A/TDI/distilled water of 2 : 1 : 1. The best adsorption is obtained with polyurethane foam added by 2.5% Chitosan. The optimum mercury adsorption 25% is resulted from the operating time of 60 minutes with adsorption capacity of 0.313 mg/g. For Chitosan modified polyurethane foam, research points out that the reaction is the second order reaction. The result concluded that the polymer has semi crystalline crystallization and melting temperatures.","PeriodicalId":17764,"journal":{"name":"Jurnal Bahan Alam Terbarukan","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"2018-07-22","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"2","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Jurnal Bahan Alam Terbarukan","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.15294/JBAT.V7I1.13614","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 2

Abstract

Mercury from the traditional gold mining activities in Aceh Jaya Regency causes water source and thus residents are exposed to mercury metals. In organic and inorganic conditions, mercury is toxic to the human body, causes damage to the nerve system, kidney failure, heart failure, blood pressure disorders, and damage to the immune system. The problem of mercury contamination can be chemically solved in various ways. This research uses polyurethane foam to adsorb mercury from water. The adsorption and selectivity of polyurethane foam adsorption can be improved through modification with Chitosan. In this research, preheating temperature, glycerol and toluene di-isocyanate (TDI) compositions greatly affect the physical form of foam. The condition under which optimal glycerol composition used for synthesizing the polyurethane foams is 20% (w/w of mixture A). This glycerol composition results in polyurethane foams with an optimum ratio of the mixture A/TDI/distilled water of 2 : 1 : 1. The best adsorption is obtained with polyurethane foam added by 2.5% Chitosan. The optimum mercury adsorption 25% is resulted from the operating time of 60 minutes with adsorption capacity of 0.313 mg/g. For Chitosan modified polyurethane foam, research points out that the reaction is the second order reaction. The result concluded that the polymer has semi crystalline crystallization and melting temperatures.
壳聚糖改性聚氨酯泡沫吸附汞离子的合成
亚齐省查亚县传统金矿开采活动产生的汞会造成水源,因此居民会接触到汞金属。在有机和无机条件下,汞对人体有毒,会对神经系统、肾衰竭、心力衰竭、血压障碍和免疫系统造成损害。汞污染的问题可以通过各种方式得到化学解决。本研究采用聚氨酯泡沫吸附水中的汞。壳聚糖改性可以提高聚氨酯泡沫的吸附性能和选择性。在本研究中,预热温度、甘油和甲苯二异氰酸酯(TDI)的组成对泡沫的物理形态有很大影响。用于合成聚氨酯泡沫的最佳甘油组合物的条件是20%(混合物A的w/w)。这种甘油组合物产生聚氨酯泡沫,其中混合物A/TDI/蒸馏水的最佳比例为2∶1∶1。加入2.5%壳聚糖的聚氨酯泡沫对吸附性能最好。汞的最佳吸附率为25%,操作时间为60分钟,吸附量为0.313mg/g。对于壳聚糖改性的聚氨酯泡沫,研究指出该反应为二级反应。结果表明,该聚合物具有半结晶结晶和熔融温度。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
自引率
0.00%
发文量
0
审稿时长
24 weeks
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信