{"title":"Activity Enhancement of P25 Titanium Dioxide by Zinc Oxide for Photocatalytic Phenol Degradation","authors":"Y. S. Kurniawan, L. Yuliati","doi":"10.9767/BCREC.16.2.10319.310-319","DOIUrl":null,"url":null,"abstract":"As a benchmark photocatalyst, P25 titanium dioxide (TiO2) nanomaterial has been widely reported for its remarkable photocatalytic activity under ultraviolet (UV) irradiation. However, approaches to further improve the photocatalytic activity of the P25 TiO2 are still required. In the present work, we reported the activity enhancement of the P25 TiO2 up to more than five times higher rate constant for phenol degradation when the P25 TiO2 was coupled with zinc oxide (ZnO). The composites were prepared by a physical mixing method of P25 TiO2 and ZnO with various weight ratios of 1:0.5, 1:1, and 1:2. The composite materials were then characterized using X-ray diffraction (XRD), diffuse-reflectance ultraviolet-visible (DR UV-vis), Fourier transform infrared (FTIR), and fluorescence spectroscopies. All the composites gave better activity than the P25 TiO2, in which the TiO2/ZnO 1:1 composite material exhibited the highest first-order reaction rate constant (0.43 h−1). This remarkable enhanced degradation rate was much higher than that of the unmodified TiO2 (0.08 h−1) and ZnO (0.13 h-1). The fluorescence study revealed that the electron-hole recombination on the P25 TiO2 could be suppressed by the ZnO, which would be the reason for such activity enhancement. A study on the effect of the scavenger showed that the hydroxyl radicals played a crucial role in the photocatalytic phenol degradation. Copyright © 2021 by Authors, Published by BCREC Group. This is an open access article under the CC BY-SA License (https://creativecommons.org/licenses/by-sa/4.0). ","PeriodicalId":46276,"journal":{"name":"Bulletin of Chemical Reaction Engineering and Catalysis","volume":"16 1","pages":"310-319"},"PeriodicalIF":1.3000,"publicationDate":"2021-06-30","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Bulletin of Chemical Reaction Engineering and Catalysis","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.9767/BCREC.16.2.10319.310-319","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q3","JCRName":"ENGINEERING, CHEMICAL","Score":null,"Total":0}
引用次数: 0
引用
批量引用
氧化锌增强P25二氧化钛光催化降解苯酚的活性
作为一种基准光催化剂,P25二氧化钛(TiO2)纳米材料在紫外线(UV)照射下具有显著的光催化活性,已被广泛报道。然而,仍然需要进一步提高P25 TiO2的光催化活性的方法。在本工作中,我们报道了当P25 TiO2与氧化锌(ZnO)偶联时,P25 TiO2的活性提高到苯酚降解速率常数的五倍以上。通过P25 TiO2和ZnO的物理混合方法制备了不同重量比为1:0.5、1:1和1:2的复合材料。然后使用X射线衍射(XRD)、漫反射紫外-可见光(DR UV-vis)、傅立叶变换红外(FTIR)和荧光光谱对复合材料进行了表征。所有的复合材料都比P25 TiO2具有更好的活性,其中TiO2/ZnO1:1复合材料表现出最高的一级反应速率常数(0.43 h-1)。这种显著增强的降解速率远高于未改性的TiO2(0.08 h-1)和ZnO(0.13 h-1)。荧光研究表明,ZnO可以抑制P25 TiO2上的电子-空穴复合,这将是这种活性增强的原因。对清除剂作用的研究表明,羟基自由基在光催化降解苯酚中起着至关重要的作用。版权所有©2021作者所有,BCREC集团出版。这是CC BY-SA许可证下的开放访问文章(https://creativecommons.org/licenses/by-sa/4.0)。
本文章由计算机程序翻译,如有差异,请以英文原文为准。