{"title":"Comparison of Water Resistance for Modified Medium-Density Fiberboard","authors":"Luis Molina Irribarra, F. Kamke, S. Leavengood","doi":"10.13073/fpj-d-22-00047","DOIUrl":null,"url":null,"abstract":"\n Commercial medium-density fiberboard (MDF) products, specifically manufactured for water resistance, were evaluated over 8 days under three water exposure regimes: 90 percent relative humidity, one-sided water spray, and one-sided wet pad. A three-cycle wet-pad and drying exposure test was also performed. Rate of swelling, extent of swelling, and irreversible thickness swelling were determined. Acetylated MDF (AMDF) had the best overall performance, followed by steam-injection pressed MDF (SMDF) and polymeric methylene-diphenyl-diisocyanate–bonded moisture-resistant MDF. The fastest rate of thickness swell and linear expansion occurred with exposure to one-sided water spray and the slowest with 90 percent relative humidity exposure. While AMDF was clearly superior after 24-hour exposure, the other MDF products were nearly identical. Significant difference in thickness swell and water absorption between moisture-resistant MDF and SMDF developed after 24 hours. Regardless of the method of water exposure, the trend of best to worst MDF performance was the same.","PeriodicalId":12387,"journal":{"name":"Forest Products Journal","volume":" ","pages":""},"PeriodicalIF":1.1000,"publicationDate":"2022-10-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Forest Products Journal","FirstCategoryId":"97","ListUrlMain":"https://doi.org/10.13073/fpj-d-22-00047","RegionNum":4,"RegionCategory":"农林科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q3","JCRName":"FORESTRY","Score":null,"Total":0}
引用次数: 0
Abstract
Commercial medium-density fiberboard (MDF) products, specifically manufactured for water resistance, were evaluated over 8 days under three water exposure regimes: 90 percent relative humidity, one-sided water spray, and one-sided wet pad. A three-cycle wet-pad and drying exposure test was also performed. Rate of swelling, extent of swelling, and irreversible thickness swelling were determined. Acetylated MDF (AMDF) had the best overall performance, followed by steam-injection pressed MDF (SMDF) and polymeric methylene-diphenyl-diisocyanate–bonded moisture-resistant MDF. The fastest rate of thickness swell and linear expansion occurred with exposure to one-sided water spray and the slowest with 90 percent relative humidity exposure. While AMDF was clearly superior after 24-hour exposure, the other MDF products were nearly identical. Significant difference in thickness swell and water absorption between moisture-resistant MDF and SMDF developed after 24 hours. Regardless of the method of water exposure, the trend of best to worst MDF performance was the same.
期刊介绍:
Forest Products Journal (FPJ) is the source of information for industry leaders, researchers, teachers, students, and everyone interested in today''s forest products industry.
The Forest Products Journal is well respected for publishing high-quality peer-reviewed technical research findings at the applied or practical level that reflect the current state of wood science and technology. Articles suitable as Technical Notes are brief notes (generally 1,200 words or less) that describe new or improved equipment or techniques; report on findings produced as by-products of major studies; or outline progress to date on long-term projects.