In vitro and In vivo Investigation of poly(lactic acid)/hydroxyapatite nanoparticle scaffold containing nandrolone decanoate for the regeneration of critical-sized bone defects

IF 1.4 Q4 NANOSCIENCE & NANOTECHNOLOGY
M. Salehi, Arman Ai, Arian Ehterami, M. Einabadi, Alireza Taslimi, Armin Ai, Hamta Akbarzadeh, G. Ameli, Saeed Farzamfar, S. Shirian, Nahal Azimi, F. Sadeghi, N. Bahrami, A. Goodarzi, J. Ai
{"title":"In vitro and In vivo Investigation of poly(lactic acid)/hydroxyapatite nanoparticle scaffold containing nandrolone decanoate for the regeneration of critical-sized bone defects","authors":"M. Salehi, Arman Ai, Arian Ehterami, M. Einabadi, Alireza Taslimi, Armin Ai, Hamta Akbarzadeh, G. Ameli, Saeed Farzamfar, S. Shirian, Nahal Azimi, F. Sadeghi, N. Bahrami, A. Goodarzi, J. Ai","doi":"10.22038/NMJ.2020.07.004","DOIUrl":null,"url":null,"abstract":"Objective(s): Bone tissue engineering is aimed at the fabrication of bone graft to ameliorate bone defects without using autografts or allografts. Materials and Methods: In the present study, the coprecipitation method was used to prepare hydroxyapatite (HA) nanoparticles containing nandrolone. To do so, 12.5, 25, and 50 mg of nandrolone were loaded into poly(lactic acid) (PLA)/nano-HA, and the freeze casting method was used to fabricate porous scaffolds. The morphology, mechanical strength, wettability, porosity, degradation, blood compatibility, and cellular response of the scaffolds were evaluated using various tests. For further investigation, the developed scaffolds were incorporated into the rat calvaria defect model, and their effects on bone healing were evaluated. Results: The obtained results indicated that the fabricated scaffolds had the approximate porosity of 80% and compress strength of 6.5 MPa. Moreover, the prepared scaffolds had appropriate hydrophilicity, weight loss, and blood compatibility. Furthermore, the histopathological findings demonstrated that the defects filled with the PLA/nano-HA scaffolds containing 25 mg nandrolone healed better compared to the other study groups.Conclusion: Therefore, it was concluded that the scaffolds containing nandrolone could be used in bone regeneration.","PeriodicalId":18933,"journal":{"name":"Nanomedicine Journal","volume":null,"pages":null},"PeriodicalIF":1.4000,"publicationDate":"2020-04-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"5","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Nanomedicine Journal","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.22038/NMJ.2020.07.004","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"NANOSCIENCE & NANOTECHNOLOGY","Score":null,"Total":0}
引用次数: 5

Abstract

Objective(s): Bone tissue engineering is aimed at the fabrication of bone graft to ameliorate bone defects without using autografts or allografts. Materials and Methods: In the present study, the coprecipitation method was used to prepare hydroxyapatite (HA) nanoparticles containing nandrolone. To do so, 12.5, 25, and 50 mg of nandrolone were loaded into poly(lactic acid) (PLA)/nano-HA, and the freeze casting method was used to fabricate porous scaffolds. The morphology, mechanical strength, wettability, porosity, degradation, blood compatibility, and cellular response of the scaffolds were evaluated using various tests. For further investigation, the developed scaffolds were incorporated into the rat calvaria defect model, and their effects on bone healing were evaluated. Results: The obtained results indicated that the fabricated scaffolds had the approximate porosity of 80% and compress strength of 6.5 MPa. Moreover, the prepared scaffolds had appropriate hydrophilicity, weight loss, and blood compatibility. Furthermore, the histopathological findings demonstrated that the defects filled with the PLA/nano-HA scaffolds containing 25 mg nandrolone healed better compared to the other study groups.Conclusion: Therefore, it was concluded that the scaffolds containing nandrolone could be used in bone regeneration.
含癸酸诺龙的聚乳酸/羟基磷灰石纳米颗粒支架在体外和体内修复临界骨缺损的研究
目的:骨组织工程的目的是在不使用自体或同种异体骨移植的情况下,通过骨移植来改善骨缺损。材料与方法:本研究采用共沉淀法制备含诺龙的羟基磷灰石(HA)纳米颗粒。为此,将12.5、25和50 mg的诺龙分别装入聚乳酸(PLA)/纳米ha中,采用冷冻铸造法制备多孔支架。通过各种测试评估支架的形态、机械强度、润湿性、孔隙度、降解性、血液相容性和细胞反应。为了进一步研究,将所制备的支架植入大鼠颅骨缺损模型,并评估其对骨愈合的影响。结果:制备的支架孔隙率约为80%,抗压强度为6.5 MPa。此外,制备的支架具有适当的亲水性、减重性和血液相容性。此外,组织病理学结果表明,与其他研究组相比,含有25 mg诺龙的PLA/纳米ha支架填充的缺陷愈合更好。结论:含诺龙支架可用于骨再生。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
Nanomedicine Journal
Nanomedicine Journal NANOSCIENCE & NANOTECHNOLOGY-
CiteScore
3.40
自引率
0.00%
发文量
0
审稿时长
12 weeks
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信