Bonding of Fused Quartz with an Aromatic Silane Compound and Acidic Functional Monomers with a Tri-n-butylborane Initiated Resin.

IF 2.5 3区 医学 Q2 DENTISTRY, ORAL SURGERY & MEDICINE
Tomoyo Okazaki, Hiroyasu Koizumi, Haruto Hiraba, Akihisa Kodaira, Takayuki Yoneyama, Hideo Matsumura
{"title":"Bonding of Fused Quartz with an Aromatic Silane Compound and Acidic Functional Monomers with a Tri-n-butylborane Initiated Resin.","authors":"Tomoyo Okazaki,&nbsp;Hiroyasu Koizumi,&nbsp;Haruto Hiraba,&nbsp;Akihisa Kodaira,&nbsp;Takayuki Yoneyama,&nbsp;Hideo Matsumura","doi":"10.3290/j.jad.a45517","DOIUrl":null,"url":null,"abstract":"<p><p>Purpose: This study evaluated the effect of an aromatic silane compound and acidic functional monomer on the bond strength of fused quartz. \nMaterials and Methods: A total of 264 disk specimens were fabricated from fused quartz for shear bond testing. Two silane compounds were used: 3-(trimethoxysilyl)propyl methacrylate (3-TMSPMA) and 3-(4-methacryloyloxyphenyl) propyltrimethoxysilane (3-MPPTS). As acidic functional monomers, 4-methacryloyloxyethyl trimellitate (4-MET) and 10-methacryloyloxydecyl dihydrogen phosphate (10-MDP) were used. The disks were primed with one of each silane compound with or without the acidic functional monomer of the same molarity. The specimens were bonded with a tri-n-butylborane (TBB) initiated luting material. The shear bond strength was determined before and after 10,000 thermocycles. Bond strength was statistically evaluated with Kruskal-Wallis, Mann-Whitney U-, and Steel- Dwass tests. To test dye penetration, the specimens were immersed in 0.5 wt% fuchsin solution for 24 h after priming with each condition, bonding, and 10,000 thermocycles. The dye penetration area was determined by observing the backside of the bonded specimen with an optical microscope. The relationship between the shear bond strength and dye penetration ratio was analyzed with Spearman’s rank correlation test. \nResults: The highest post-thermocycling bond strengths in the 1 mol% and 2 mol% groups were 3-TMSPMA + 10- MDP and 3-MPPTS + 10-MDP. Spearman’s rank correlation coefficient between shear bond strength and dye penetration area was γ = -0.7519, indicating a strong negative correlation. \nConclusion: The surface treatments of 3-TMSPMA and 3-MPPTS combined with 10-MDP yielded higher bond strength after 10,000 thermocycles than those combined with 4-MET, despite the similarity in molarity. The shear bond strength was negatively correlated with the dye penetration area.</p>","PeriodicalId":55604,"journal":{"name":"Journal of Adhesive Dentistry","volume":"22 6","pages":"615-624"},"PeriodicalIF":2.5000,"publicationDate":"2020-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Adhesive Dentistry","FirstCategoryId":"3","ListUrlMain":"https://doi.org/10.3290/j.jad.a45517","RegionNum":3,"RegionCategory":"医学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q2","JCRName":"DENTISTRY, ORAL SURGERY & MEDICINE","Score":null,"Total":0}
引用次数: 0

Abstract

Purpose: This study evaluated the effect of an aromatic silane compound and acidic functional monomer on the bond strength of fused quartz. Materials and Methods: A total of 264 disk specimens were fabricated from fused quartz for shear bond testing. Two silane compounds were used: 3-(trimethoxysilyl)propyl methacrylate (3-TMSPMA) and 3-(4-methacryloyloxyphenyl) propyltrimethoxysilane (3-MPPTS). As acidic functional monomers, 4-methacryloyloxyethyl trimellitate (4-MET) and 10-methacryloyloxydecyl dihydrogen phosphate (10-MDP) were used. The disks were primed with one of each silane compound with or without the acidic functional monomer of the same molarity. The specimens were bonded with a tri-n-butylborane (TBB) initiated luting material. The shear bond strength was determined before and after 10,000 thermocycles. Bond strength was statistically evaluated with Kruskal-Wallis, Mann-Whitney U-, and Steel- Dwass tests. To test dye penetration, the specimens were immersed in 0.5 wt% fuchsin solution for 24 h after priming with each condition, bonding, and 10,000 thermocycles. The dye penetration area was determined by observing the backside of the bonded specimen with an optical microscope. The relationship between the shear bond strength and dye penetration ratio was analyzed with Spearman’s rank correlation test. Results: The highest post-thermocycling bond strengths in the 1 mol% and 2 mol% groups were 3-TMSPMA + 10- MDP and 3-MPPTS + 10-MDP. Spearman’s rank correlation coefficient between shear bond strength and dye penetration area was γ = -0.7519, indicating a strong negative correlation. Conclusion: The surface treatments of 3-TMSPMA and 3-MPPTS combined with 10-MDP yielded higher bond strength after 10,000 thermocycles than those combined with 4-MET, despite the similarity in molarity. The shear bond strength was negatively correlated with the dye penetration area.

熔融石英与芳香硅烷化合物及酸性功能单体与三丁基硼烷引发树脂的键合。
目的:研究芳香硅烷化合物和酸性功能单体对熔融石英粘结强度的影响。材料与方法:用熔融石英制作了264个圆盘试样进行剪切粘接试验。使用了两种硅烷化合物:3-(三甲氧基硅基)甲基丙烯酸丙酯(3- tmspma)和3-(4-甲基丙烯酰氧基苯基)丙基三甲氧基硅烷(3- mppts)。酸性功能单体为4-甲基丙烯酰氧乙基三ellate (4-MET)和10-甲基丙烯酰氧癸基磷酸二氢(10-MDP)。在圆盘上分别引入具有或不具有相同摩尔浓度的酸性功能单体的硅烷化合物。样品与三丁基硼烷(TBB)引发的粘结材料结合。在10,000次热循环前后测定剪切粘结强度。结合强度用Kruskal-Wallis、Mann-Whitney U和Steel- Dwass检验进行统计评价。为了测试染料的渗透,在每种条件下进行底漆、粘合和10,000次热循环后,将样品浸入0.5 wt%的品红溶液中24小时。用光学显微镜观察粘接试样的背面,确定染料穿透面积。采用Spearman秩相关检验分析剪切结合强度与染料穿透率的关系。结果:1 mol%组和2 mol%组的热循环后黏结强度最高的是3-TMSPMA + 10-MDP和3-MPPTS + 10-MDP。剪切结合强度与染料穿透面积的Spearman等级相关系数为γ = -0.7519,呈较强的负相关。结论:3-TMSPMA和3-MPPTS与10-MDP结合的表面处理在10000次热循环后的结合强度高于与4-MET结合的表面处理,尽管它们的摩尔浓度相似。剪切结合强度与染料渗透面积呈负相关。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
Journal of Adhesive Dentistry
Journal of Adhesive Dentistry 医学-牙科与口腔外科
CiteScore
5.20
自引率
6.10%
发文量
44
审稿时长
6-12 weeks
期刊介绍: New materials and applications for adhesion are profoundly changing the way dentistry is delivered. Bonding techniques, which have long been restricted to the tooth hard tissues, enamel, and dentin, have obvious applications in operative and preventive dentistry, as well as in esthetic and pediatric dentistry, prosthodontics, and orthodontics. The current development of adhesive techniques for soft tissues and slow-releasing agents will expand applications to include periodontics and oral surgery. Scientifically sound, peer-reviewed articles explore the latest innovations in these emerging fields.
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信