The effect of different re-mineralizing agents and diode laser irradiation on the microhardness of primary molar enamel: An in vitro study.

Q2 Medicine
Zahra Bahrololoomi, Fatemeh Zarebidoki, Nasrin Mostafalu
{"title":"The effect of different re-mineralizing agents and diode laser irradiation on the microhardness of primary molar enamel: An <i>in vitro</i> study.","authors":"Zahra Bahrololoomi,&nbsp;Fatemeh Zarebidoki,&nbsp;Nasrin Mostafalu","doi":"10.5978/islsm.28_19-OR-15","DOIUrl":null,"url":null,"abstract":"<p><strong>Background and aims: </strong>Dental caries is a global concern and different materials and methods were proposed for its prevention.The aim of this study was evaluation of the effect of different demineralizing agents with and without diode laser radiation on the microhardness of primary molars enamel.</p><p><strong>Materials and methods: </strong>48 primary molar teeth were used in this study. The enamel blocks were prepared. Primary microhardness values were also measured. All samples were demineralized, then demineralization was approved by a DIAGNOdent pen. The remineralization was done into the buccal and lingual surfaces of the samples as follows:Group 1: CPP-ACP, Group 2: CPP-ACPF, Group 3: MI varnish, Group 4: NaF varnish. The lingual surfaces received diode laser irradiation. Finally, a secondary microhardness test was performed on all samples. Statistical analyses were done and a P-value less than 0.05 was considered to be statistically significant.</p><p><strong>Results: </strong>A comparison between the primary and the secondary microhardness values showed significant differences (P = 0.003). The highest secondary microhardness values belonged to the MI varnish +laser group.</p><p><strong>Conclusion: </strong>Application of the agents, containing the combination of Ca, P, and F, was significantly better than others in increasing the microhardness of the enamel. Although the application of diode laser increased the hardness of the enamel.</p>","PeriodicalId":17981,"journal":{"name":"Laser therapy","volume":"28 3","pages":"187-192"},"PeriodicalIF":0.0000,"publicationDate":"2019-09-30","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://sci-hub-pdf.com/10.5978/islsm.28_19-OR-15","citationCount":"3","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Laser therapy","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.5978/islsm.28_19-OR-15","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q2","JCRName":"Medicine","Score":null,"Total":0}
引用次数: 3

Abstract

Background and aims: Dental caries is a global concern and different materials and methods were proposed for its prevention.The aim of this study was evaluation of the effect of different demineralizing agents with and without diode laser radiation on the microhardness of primary molars enamel.

Materials and methods: 48 primary molar teeth were used in this study. The enamel blocks were prepared. Primary microhardness values were also measured. All samples were demineralized, then demineralization was approved by a DIAGNOdent pen. The remineralization was done into the buccal and lingual surfaces of the samples as follows:Group 1: CPP-ACP, Group 2: CPP-ACPF, Group 3: MI varnish, Group 4: NaF varnish. The lingual surfaces received diode laser irradiation. Finally, a secondary microhardness test was performed on all samples. Statistical analyses were done and a P-value less than 0.05 was considered to be statistically significant.

Results: A comparison between the primary and the secondary microhardness values showed significant differences (P = 0.003). The highest secondary microhardness values belonged to the MI varnish +laser group.

Conclusion: Application of the agents, containing the combination of Ca, P, and F, was significantly better than others in increasing the microhardness of the enamel. Although the application of diode laser increased the hardness of the enamel.

不同再矿化剂及二极管激光照射对一磨牙釉质显微硬度的影响。
背景与目的:龋齿是一个全球性的问题,人们提出了不同的预防材料和方法。本研究的目的是评价不同的脱矿剂在二极管激光照射和不照射下对初级磨牙牙釉质显微硬度的影响。材料和方法:本研究使用48颗乳牙。搪瓷块准备好了。测定了初级显微硬度值。所有样品均进行脱矿处理,然后由诊断笔批准脱矿。在口腔和舌面进行再矿化处理:组1:CPP-ACP,组2:CPP-ACPF,组3:MI清漆,组4:NaF清漆。舌面接受二极管激光照射。最后,对所有样品进行二次显微硬度测试。进行统计学分析,认为p值小于0.05具有统计学意义。结果:初级显微硬度值与次级显微硬度值比较差异有统计学意义(P = 0.003)。MI清漆+激光组的二次显微硬度值最高。结论:Ca、P、F复合制剂对提高牙釉质显微硬度的效果明显优于其他制剂。虽然二极管激光的应用增加了牙釉质的硬度。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
Laser therapy
Laser therapy Medicine-Surgery
CiteScore
2.80
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信