Dimensional stability of two impression materials after a 6-month storage period.

Acta Biomaterialia Odontologica Scandinavica Pub Date : 2017-11-14 eCollection Date: 2017-01-01 DOI:10.1080/23337931.2017.1401933
Francisco Martins, Patrícia Branco, José Reis, Ignacio Barbero Navarro, Paulo Maurício
{"title":"Dimensional stability of two impression materials after a 6-month storage period.","authors":"Francisco Martins,&nbsp;Patrícia Branco,&nbsp;José Reis,&nbsp;Ignacio Barbero Navarro,&nbsp;Paulo Maurício","doi":"10.1080/23337931.2017.1401933","DOIUrl":null,"url":null,"abstract":"<p><p><b>Objective:</b> Oral rehabilitation success is enhanced by an accurate and reproducible final impression. The purpose of this study is to evaluate the dimensional changes of a polyether and addition silicone subjected to disinfection and/or sterilization after a long storage period. <b>Material and methods:</b> Ninety samples were obtained from polyether Impregum<sup>TM</sup> Penta<sup>TM</sup> (3M ESPE<sup>TM</sup>, Seefeld, Germany) and 90 of addition silicone Imprint<sup>TM</sup> 4 Penta<sup>TM</sup> Putty (3M ESPE<sup>TM</sup>, Seefeld, Germany) according to ISO 4823:2000. The samples of each material were split to form three groups with 30 samples each: a control group, a hypochlorite group (disinfection) and an autoclave group (sterilization). Samples were stored in the Portuguese Institute for Quality for six months at 23 °C. Samples were measured by laser interferometry, according to the Michelson technique before calculating dimensional stability according ISO 4823:2000. A statistical analysis via a three-way mixed ANOVA was performed. <b>Results:</b> Significant shrinkage of Impregum<sup>TM</sup> Penta<sup>TM</sup> was 0.77 ± 0.17% in the control group, 0.42 ± 0.19% in the hypochlorite group and 0.52 ± 0.28% in the autoclave group. For Imprint<sup>TM</sup> 4 Penta<sup>TM</sup> Putty, the control group had a shrinkage of 0.42 ± 0.12%, the hypochlorite group 0.36 ± 0.09% and the autoclave group 0.59 ± 0.13%. <b>Conclusions:</b> The long-term storage of samples subjected to disinfection with 5.25% hypochlorite or autoclave sterilization can be used in a clinical setting as the dimensional changes are below the maximum permitted by the ISO 4823:2000, since there are no clinically significant changes in the dimension of the samples during the storage period.</p>","PeriodicalId":6997,"journal":{"name":"Acta Biomaterialia Odontologica Scandinavica","volume":"3 1","pages":"84-91"},"PeriodicalIF":0.0000,"publicationDate":"2017-11-14","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://sci-hub-pdf.com/10.1080/23337931.2017.1401933","citationCount":"8","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Acta Biomaterialia Odontologica Scandinavica","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1080/23337931.2017.1401933","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"2017/1/1 0:00:00","PubModel":"eCollection","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 8

Abstract

Objective: Oral rehabilitation success is enhanced by an accurate and reproducible final impression. The purpose of this study is to evaluate the dimensional changes of a polyether and addition silicone subjected to disinfection and/or sterilization after a long storage period. Material and methods: Ninety samples were obtained from polyether ImpregumTM PentaTM (3M ESPETM, Seefeld, Germany) and 90 of addition silicone ImprintTM 4 PentaTM Putty (3M ESPETM, Seefeld, Germany) according to ISO 4823:2000. The samples of each material were split to form three groups with 30 samples each: a control group, a hypochlorite group (disinfection) and an autoclave group (sterilization). Samples were stored in the Portuguese Institute for Quality for six months at 23 °C. Samples were measured by laser interferometry, according to the Michelson technique before calculating dimensional stability according ISO 4823:2000. A statistical analysis via a three-way mixed ANOVA was performed. Results: Significant shrinkage of ImpregumTM PentaTM was 0.77 ± 0.17% in the control group, 0.42 ± 0.19% in the hypochlorite group and 0.52 ± 0.28% in the autoclave group. For ImprintTM 4 PentaTM Putty, the control group had a shrinkage of 0.42 ± 0.12%, the hypochlorite group 0.36 ± 0.09% and the autoclave group 0.59 ± 0.13%. Conclusions: The long-term storage of samples subjected to disinfection with 5.25% hypochlorite or autoclave sterilization can be used in a clinical setting as the dimensional changes are below the maximum permitted by the ISO 4823:2000, since there are no clinically significant changes in the dimension of the samples during the storage period.

Abstract Image

Abstract Image

Abstract Image

两种压印材料储存6个月后的尺寸稳定性。
目的:准确、可重复的最终印模可提高口腔康复成功率。本研究的目的是评价聚醚和添加有机硅经过长期储存消毒和/或灭菌后的尺寸变化。材料和方法:根据ISO 4823:2000,从聚醚ImpregumTM PentaTM (3M ESPETM, Seefeld, Germany)和90个添加硅酮ImprintTM 4 PentaTM腻子(3M ESPETM, Seefeld, Germany)中获得样品。每种材料的样品被分成三组,每组30个样品:对照组,次氯酸盐组(消毒)和高压灭菌组(灭菌)。样品在葡萄牙质量研究所保存6个月,温度23°C。在根据ISO 4823:2000计算尺寸稳定性之前,根据迈克尔逊技术,用激光干涉测量法测量样品。通过三向混合方差分析进行统计分析。结果:ImpregumTM PentaTM的收缩率在对照组为0.77±0.17%,次氯酸盐组为0.42±0.19%,高压釜组为0.52±0.28%。对于imprinttm4pentatm腻子,对照组收缩率为0.42±0.12%,次氯酸盐组为0.36±0.09%,高压灭菌组为0.59±0.13%。结论:经5.25%次氯酸盐或高压灭菌器消毒后的样品长期存放,由于样品在存放期间尺寸变化小于ISO 4823:2000允许的最大尺寸变化,因此可用于临床。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信