Effect of surface sealing on stain resistance of a nano-hybrid resin composite.

Journal of Istanbul University Faculty of Dentistry Pub Date : 2015-04-29 eCollection Date: 2015-01-01 DOI:10.17096/jiufd.24298
Gunce Saygi, Pinar Karakoc, Isil Serbes, Ugur Erdemir, Taner Yucel
{"title":"Effect of surface sealing on stain resistance of a nano-hybrid resin composite.","authors":"Gunce Saygi,&nbsp;Pinar Karakoc,&nbsp;Isil Serbes,&nbsp;Ugur Erdemir,&nbsp;Taner Yucel","doi":"10.17096/jiufd.24298","DOIUrl":null,"url":null,"abstract":"<p><strong>Purpose: </strong>This study investigated the influence of sealant application on stain resistance of a nanohybrid resin composite compared to the efficacy of a bonding agent used as a surface sealant on prolonging color stability of the resin composite.</p><p><strong>Materials and methods: </strong>28 disc-shaped materials were prepared from a nano-hybrid resin composite Filtek Z550 and assigned to four groups: G1K: nonsealed; G2:Adper Single Bond; G3: Fortify ; G4: Biscover LV. After 24 h storage in distilled water at 37˚C, all specimens were subjected to thermocycling and immersed into coffee solution. Color measurements were performed using spectrophotometer (VITA Easyshade; Vident) according to CIEL*a*b* system.</p><p><strong>Results: </strong>Color change values were significantly different among the groups in each evaluation period except for after thermocycling (p<0.05). For 7 days evaluation period, the difference between G3 and G4 group was statistically significant while G4 exhibited statistically significant differences (p<0.05 and p<0.0001 respectively) compared to control (G1) in 14 day whereas no significant difference was found between GI and GII in 28-day evaluation period. However, ΔE values of sealed specimens (GIII, GIV) differed significantly from non-sealed (GI) specimens after 28 days of immersion in coffee solution (p<0.05 and p<0.0001 respectively).</p><p><strong>Conclusion: </strong>It may be concluded that using a bonding agent as a surface sealant does not increase stain resistance of resin composites of the sealants evaluated. Biscover LV showed the highest efficacy to prolong color stability of the resin composite.</p>","PeriodicalId":30947,"journal":{"name":"Journal of Istanbul University Faculty of Dentistry","volume":"49 2","pages":"23-30"},"PeriodicalIF":0.0000,"publicationDate":"2015-04-29","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://ftp.ncbi.nlm.nih.gov/pub/pmc/oa_pdf/ff/11/jiufd-049-023.PMC5573481.pdf","citationCount":"5","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Istanbul University Faculty of Dentistry","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.17096/jiufd.24298","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"2015/1/1 0:00:00","PubModel":"eCollection","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 5

Abstract

Purpose: This study investigated the influence of sealant application on stain resistance of a nanohybrid resin composite compared to the efficacy of a bonding agent used as a surface sealant on prolonging color stability of the resin composite.

Materials and methods: 28 disc-shaped materials were prepared from a nano-hybrid resin composite Filtek Z550 and assigned to four groups: G1K: nonsealed; G2:Adper Single Bond; G3: Fortify ; G4: Biscover LV. After 24 h storage in distilled water at 37˚C, all specimens were subjected to thermocycling and immersed into coffee solution. Color measurements were performed using spectrophotometer (VITA Easyshade; Vident) according to CIEL*a*b* system.

Results: Color change values were significantly different among the groups in each evaluation period except for after thermocycling (p<0.05). For 7 days evaluation period, the difference between G3 and G4 group was statistically significant while G4 exhibited statistically significant differences (p<0.05 and p<0.0001 respectively) compared to control (G1) in 14 day whereas no significant difference was found between GI and GII in 28-day evaluation period. However, ΔE values of sealed specimens (GIII, GIV) differed significantly from non-sealed (GI) specimens after 28 days of immersion in coffee solution (p<0.05 and p<0.0001 respectively).

Conclusion: It may be concluded that using a bonding agent as a surface sealant does not increase stain resistance of resin composites of the sealants evaluated. Biscover LV showed the highest efficacy to prolong color stability of the resin composite.

表面密封对纳米杂化树脂复合材料耐污性能的影响。
目的:研究密封胶对纳米杂化树脂复合材料耐污性的影响,并与表面密封胶结合剂对树脂复合材料颜色稳定性的影响进行比较。材料与方法:采用Filtek Z550纳米复合树脂制备28种圆盘状材料,分为4组:G1K:非密封;G2:Adper单键;G3:加固;发现LV。在37˚C蒸馏水中保存24 h后,所有样品进行热循环并浸入咖啡溶液中。颜色测量采用分光光度计(VITA Easyshade;根据CIEL*a*b*系统。结果:除热循环后外,各组在各评价时期的颜色变化值均有显著差异(p)。结论:可以认为,使用粘结剂作为表面密封胶并不会增加所评价密封胶的树脂复合材料的耐污性。Biscover LV对树脂复合材料颜色稳定性的延长效果最好。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
自引率
0.00%
发文量
0
审稿时长
12 weeks
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信