{"title":"Influence of load, sliding speed, and temperature on the tribological behavior of plasma sprayed BaF2-doped YSZ composite coatings","authors":"Rajib Das, P.P. Bandyopadhyay","doi":"10.1016/j.jeurceramsoc.2025.117476","DOIUrl":null,"url":null,"abstract":"<div><div>This report explores the tribological characteristics of BaF<sub>2</sub>-doped YSZ coatings under varying loads, speeds, and temperatures. Up to 10 N load, the friction coefficient (COF) decreases owing to elastic contact, then it stabilizes within 0.78 – 0.80 as plastic contact dominates. At 650 °C, BaF<sub>2</sub> extrusion under high loads reduces the COF to 0.56. Increased speed further lowers the COF through debris ejection and asperity softening. The wear rate rises with load and speed owing to Hertzian stress and tangential impact, respectively. Fatigue and abrasive wear are the main wear mechanisms. BaF<sub>2</sub> layer provides significant wear protection, and with temperature, its shear strength reduces, lowering the COF to 0.39 and wear rate to 5.36 × 10<sup>−4</sup> mm<sup>3</sup>/Nm at 750 °C.</div></div>","PeriodicalId":17408,"journal":{"name":"Journal of The European Ceramic Society","volume":"45 13","pages":"Article 117476"},"PeriodicalIF":5.8000,"publicationDate":"2025-04-22","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of The European Ceramic Society","FirstCategoryId":"88","ListUrlMain":"https://www.sciencedirect.com/science/article/pii/S0955221925002961","RegionNum":2,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q1","JCRName":"MATERIALS SCIENCE, CERAMICS","Score":null,"Total":0}
引用次数: 0
Abstract
This report explores the tribological characteristics of BaF2-doped YSZ coatings under varying loads, speeds, and temperatures. Up to 10 N load, the friction coefficient (COF) decreases owing to elastic contact, then it stabilizes within 0.78 – 0.80 as plastic contact dominates. At 650 °C, BaF2 extrusion under high loads reduces the COF to 0.56. Increased speed further lowers the COF through debris ejection and asperity softening. The wear rate rises with load and speed owing to Hertzian stress and tangential impact, respectively. Fatigue and abrasive wear are the main wear mechanisms. BaF2 layer provides significant wear protection, and with temperature, its shear strength reduces, lowering the COF to 0.39 and wear rate to 5.36 × 10−4 mm3/Nm at 750 °C.
期刊介绍:
The Journal of the European Ceramic Society publishes the results of original research and reviews relating to ceramic materials. Papers of either an experimental or theoretical character will be welcomed on a fully international basis. The emphasis is on novel generic science concerning the relationships between processing, microstructure and properties of polycrystalline ceramics consolidated at high temperature. Papers may relate to any of the conventional categories of ceramic: structural, functional, traditional or composite. The central objective is to sustain a high standard of research quality by means of appropriate reviewing procedures.