Laser welding of dissimilar TiAl/Ti6-Al-4V materials: Effects of rapid in-situ laser pre-heating on microstructure and mechanical properties of the welding joint
Qiyuan Yu , Yu Zhang , Ziyuan Jia , Lujun Huang , Lin Geng , Liqun Li
{"title":"Laser welding of dissimilar TiAl/Ti6-Al-4V materials: Effects of rapid in-situ laser pre-heating on microstructure and mechanical properties of the welding joint","authors":"Qiyuan Yu , Yu Zhang , Ziyuan Jia , Lujun Huang , Lin Geng , Liqun Li","doi":"10.1016/j.intermet.2024.108514","DOIUrl":null,"url":null,"abstract":"<div><div>TiAl alloy has broad application prospects in the aerospace field. In practical working environments, connecting with other materials is considered an important means of fully utilizing their excellent properties. This study employed a laser in-situ pre-scanning method to preheat the weld seam, achieving the connection between TiAl alloy and Ti-6Al-4V. On this basis, the microstructural evolution of the fusion zone (FZ), fusion line (FL), and heat-affected zone (HAZ) of the welded joint was analyzed in detail. By comparing with traditional welding processes, the effects of laser in-situ preheating on the microstructure and properties of the welded joints were studied. The results showed that the FZ area consists of α<sub>2</sub> and martensitic α-Ti, while the FL on the TiAl side features a transition layer of β/B2 phases, providing plasticity and toughness to the welded joint. The in-situ scanning method reduced the cracks generated during welding, resulting in a more uniform distribution of the transition layer. The obtained FZ exhibited higher microhardness. The room temperature tensile strength of the welded joint reached 650 MPa. As the temperature increased, at 400 °C, the tensile strength and elongation reached 571 MPa and 3 %, respectively, significantly higher than the 450 MPa and 1.5 % achieved by conventional welding at the same temperature. When the temperature further increased to 500 °C and 600 °C, Ti-6Al-4V experienced significant softening, becoming the weak point of the welded joint.</div></div>","PeriodicalId":331,"journal":{"name":"Intermetallics","volume":"175 ","pages":"Article 108514"},"PeriodicalIF":4.3000,"publicationDate":"2024-10-19","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Intermetallics","FirstCategoryId":"88","ListUrlMain":"https://www.sciencedirect.com/science/article/pii/S0966979524003339","RegionNum":2,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q2","JCRName":"CHEMISTRY, PHYSICAL","Score":null,"Total":0}
引用次数: 0
Abstract
TiAl alloy has broad application prospects in the aerospace field. In practical working environments, connecting with other materials is considered an important means of fully utilizing their excellent properties. This study employed a laser in-situ pre-scanning method to preheat the weld seam, achieving the connection between TiAl alloy and Ti-6Al-4V. On this basis, the microstructural evolution of the fusion zone (FZ), fusion line (FL), and heat-affected zone (HAZ) of the welded joint was analyzed in detail. By comparing with traditional welding processes, the effects of laser in-situ preheating on the microstructure and properties of the welded joints were studied. The results showed that the FZ area consists of α2 and martensitic α-Ti, while the FL on the TiAl side features a transition layer of β/B2 phases, providing plasticity and toughness to the welded joint. The in-situ scanning method reduced the cracks generated during welding, resulting in a more uniform distribution of the transition layer. The obtained FZ exhibited higher microhardness. The room temperature tensile strength of the welded joint reached 650 MPa. As the temperature increased, at 400 °C, the tensile strength and elongation reached 571 MPa and 3 %, respectively, significantly higher than the 450 MPa and 1.5 % achieved by conventional welding at the same temperature. When the temperature further increased to 500 °C and 600 °C, Ti-6Al-4V experienced significant softening, becoming the weak point of the welded joint.
期刊介绍:
This journal is a platform for publishing innovative research and overviews for advancing our understanding of the structure, property, and functionality of complex metallic alloys, including intermetallics, metallic glasses, and high entropy alloys.
The journal reports the science and engineering of metallic materials in the following aspects:
Theories and experiments which address the relationship between property and structure in all length scales.
Physical modeling and numerical simulations which provide a comprehensive understanding of experimental observations.
Stimulated methodologies to characterize the structure and chemistry of materials that correlate the properties.
Technological applications resulting from the understanding of property-structure relationship in materials.
Novel and cutting-edge results warranting rapid communication.
The journal also publishes special issues on selected topics and overviews by invitation only.