Tailored Casting and Hot Rolling Temperatures for the Preparation of Hot Stamping Steel Thin Strip

Renyi Yang, Wanlin Wang, Chenyang Zhu, Jie Zeng
{"title":"Tailored Casting and Hot Rolling Temperatures for the Preparation of Hot Stamping Steel Thin Strip","authors":"Renyi Yang, Wanlin Wang, Chenyang Zhu, Jie Zeng","doi":"10.1007/s11663-024-03269-x","DOIUrl":null,"url":null,"abstract":"<p>Strip casting casts molten steel into thin strips, enabling direct hot rolling to produce products. A typical hot stamping steel thin strip was made by a strip casting simulator under tailored casting and hot rolling temperatures. The casting strip showed improved surface quality at a higher casting temperature (1597 °C) and a lower rolling temperature (900 °C), achieving 1275 MPa tensile strength with 12.3 pct elongation due to refined austenite grains transforming to martensite.</p>","PeriodicalId":18613,"journal":{"name":"Metallurgical and Materials Transactions B","volume":"94 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2024-09-13","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Metallurgical and Materials Transactions B","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1007/s11663-024-03269-x","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

Strip casting casts molten steel into thin strips, enabling direct hot rolling to produce products. A typical hot stamping steel thin strip was made by a strip casting simulator under tailored casting and hot rolling temperatures. The casting strip showed improved surface quality at a higher casting temperature (1597 °C) and a lower rolling temperature (900 °C), achieving 1275 MPa tensile strength with 12.3 pct elongation due to refined austenite grains transforming to martensite.

Abstract Image

用于制备热冲压钢薄板的定制铸造和热轧温度
带钢铸造将钢水浇铸成薄钢带,然后直接进行热轧生产产品。带钢铸造模拟器在定制的铸造和热轧温度下制造了典型的热冲压薄钢带。在较高的铸造温度(1597 °C)和较低的轧制温度(900 °C)下,铸造钢带的表面质量得到改善,由于精奥氏体晶粒转变为马氏体,抗拉强度达到 1275 兆帕,伸长率为 12.3%。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信