{"title":"Delayed fracture of ion-exchange strengthened alkali-aluminosilicate glass","authors":"Jared S. Aaldenberg, Marvin W. Kemmerer, James E. Webb","doi":"10.1111/jace.19993","DOIUrl":null,"url":null,"abstract":"<p>Delayed fracture occurs when cracks grow subcritically prior to achieving <i>K</i><sub>IC</sub>. Glass science research in this area has focused almost exclusively on non ion-exchanged glasses. In this study, an ion-exchange strengthened aluminosilicate glass was intentionally damaged to measure delayed fracture behavior. Damage was applied both pre and post ion-exchange and the role of heat-treatments was investigated. It was found that the delayed fracture likelihood was reduced for samples that were heat-treated in an environment containing water vapor. An increase in the static fatigue limit was measured for increasing temperature and it was hypothesized that crack toughening takes place during the heat-treatment due to a water-assisted stress relaxation mechanism.</p>","PeriodicalId":200,"journal":{"name":"Journal of the American Ceramic Society","volume":"107 12","pages":"8061-8070"},"PeriodicalIF":3.5000,"publicationDate":"2024-08-21","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of the American Ceramic Society","FirstCategoryId":"88","ListUrlMain":"https://onlinelibrary.wiley.com/doi/10.1111/jace.19993","RegionNum":3,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q1","JCRName":"MATERIALS SCIENCE, CERAMICS","Score":null,"Total":0}
引用次数: 0
Abstract
Delayed fracture occurs when cracks grow subcritically prior to achieving KIC. Glass science research in this area has focused almost exclusively on non ion-exchanged glasses. In this study, an ion-exchange strengthened aluminosilicate glass was intentionally damaged to measure delayed fracture behavior. Damage was applied both pre and post ion-exchange and the role of heat-treatments was investigated. It was found that the delayed fracture likelihood was reduced for samples that were heat-treated in an environment containing water vapor. An increase in the static fatigue limit was measured for increasing temperature and it was hypothesized that crack toughening takes place during the heat-treatment due to a water-assisted stress relaxation mechanism.
期刊介绍:
The Journal of the American Ceramic Society contains records of original research that provide insight into or describe the science of ceramic and glass materials and composites based on ceramics and glasses. These papers include reports on discovery, characterization, and analysis of new inorganic, non-metallic materials; synthesis methods; phase relationships; processing approaches; microstructure-property relationships; and functionalities. Of great interest are works that support understanding founded on fundamental principles using experimental, theoretical, or computational methods or combinations of those approaches. All the published papers must be of enduring value and relevant to the science of ceramics and glasses or composites based on those materials.
Papers on fundamental ceramic and glass science are welcome including those in the following areas:
Enabling materials for grand challenges[...]
Materials design, selection, synthesis and processing methods[...]
Characterization of compositions, structures, defects, and properties along with new methods [...]
Mechanisms, Theory, Modeling, and Simulation[...]
JACerS accepts submissions of full-length Articles reporting original research, in-depth Feature Articles, Reviews of the state-of-the-art with compelling analysis, and Rapid Communications which are short papers with sufficient novelty or impact to justify swift publication.