A novel material selection method and application in an aqueous environment containing CO2, H2S, O2, and SO2

Kexi Liao, Jihui Leng, Yongbo Yan, T. He, Xidi Lv, Xin Liu, Min Qin, Shuai Zhao, Y. F. Cheng
{"title":"A novel material selection method and application in an aqueous environment containing CO2, H2S, O2, and SO2","authors":"Kexi Liao, Jihui Leng, Yongbo Yan, T. He, Xidi Lv, Xin Liu, Min Qin, Shuai Zhao, Y. F. Cheng","doi":"10.1177/1478422x231221061","DOIUrl":null,"url":null,"abstract":"The corrosion in the aqueous environment of CO2–H2S–O2–SO2 is extremely severe, causing frequent failures of pipeline and posing a challenging issue for material selection. This paper drew on excellent standards and past experiences to provide a suitable method for selecting materials. The method consisted of four components: standard primary selection, corrosion evaluation selection, mechanical property selection, and economic final selection. A case study demonstrated that the applicable materials for the environment (total pressure of 1.5 MPa, temperature of 30–120 °C, H2S content of 0.1–1.5%, CO2 content of 8–55%, SO2 content of 0–0.00015% and O2 content of 1–3%) were composed of 2Cr13 or 316L. Additionally, the main control factors for corrosion rate were ranked as follows: O2 > H2S > temperature > CO2 > SO2. And a reduction in mechanical properties was observed for 2Cr13, 316L, and 825 after corrosion.","PeriodicalId":517061,"journal":{"name":"Corrosion Engineering, Science and Technology: The International Journal of Corrosion Processes and Corrosion Control","volume":"31 4","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2024-01-15","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Corrosion Engineering, Science and Technology: The International Journal of Corrosion Processes and Corrosion Control","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1177/1478422x231221061","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

The corrosion in the aqueous environment of CO2–H2S–O2–SO2 is extremely severe, causing frequent failures of pipeline and posing a challenging issue for material selection. This paper drew on excellent standards and past experiences to provide a suitable method for selecting materials. The method consisted of four components: standard primary selection, corrosion evaluation selection, mechanical property selection, and economic final selection. A case study demonstrated that the applicable materials for the environment (total pressure of 1.5 MPa, temperature of 30–120 °C, H2S content of 0.1–1.5%, CO2 content of 8–55%, SO2 content of 0–0.00015% and O2 content of 1–3%) were composed of 2Cr13 or 316L. Additionally, the main control factors for corrosion rate were ranked as follows: O2 > H2S > temperature > CO2 > SO2. And a reduction in mechanical properties was observed for 2Cr13, 316L, and 825 after corrosion.
新型材料选择方法及在含 CO2、H2S、O2 和 SO2 的水环境中的应用
CO2-H2S-O2-SO2 的水环境腐蚀极为严重,导致管道故障频发,给材料选择带来了挑战。本文借鉴了优秀标准和以往经验,提供了一种合适的材料选择方法。该方法由四个部分组成:标准初选、腐蚀评估选择、机械性能选择和经济性终选。案例研究表明,适用于该环境(总压为 1.5 兆帕、温度为 30-120 °C、H2S 含量为 0.1-1.5%、CO2 含量为 8-55%、SO2 含量为 0-0.00015% 和 O2 含量为 1-3%)的材料由 2Cr13 或 316L 组成。此外,腐蚀速率的主要控制因素排序如下:O2 > H2S > 温度 > CO2 > SO2。此外,还观察到 2Cr13、316L 和 825 在腐蚀后的机械性能有所下降。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信