The effect of calcium oxide addition from feather clam shells on porosity and water adsorption geopolymer composite bricks

N. Nurfajriani, Yohansen Wahyudi
{"title":"The effect of calcium oxide addition from feather clam shells on porosity and water adsorption geopolymer composite bricks","authors":"N. Nurfajriani, Yohansen Wahyudi","doi":"10.24114/jpkim.v15i3.50903","DOIUrl":null,"url":null,"abstract":"The purpose of this study was to study the effect of adding CaO (calcium oxide) from clam shell ash on physical properties such as density, porosity and water absorption on geopolymer composite bricks. Geopolymer composite bricks are made by mixing sand, geopolymers synthesized from fly ash with NaOH and Na2SiO3 and calcium oxide calcined from feather clam shell which is printed in cylinder form. The bricks are then cured for 28 days and physical tests are carried out in the form of density, water absorption and porosity tests. The results showed that the most optimal addition of CaO is 7.5% for the physical properties of geopolymer composite bricks with a density value of 1.80 gr/cm3, a porosity value of 10.30% and a water absorption capacity of 4.68%. The value has filled the quality standard 1st for bricks set by Indonesian National Standard (SNI).","PeriodicalId":17697,"journal":{"name":"Jurnal Pendidikan Kimia","volume":"62 4","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2023-12-08","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Jurnal Pendidikan Kimia","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.24114/jpkim.v15i3.50903","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

The purpose of this study was to study the effect of adding CaO (calcium oxide) from clam shell ash on physical properties such as density, porosity and water absorption on geopolymer composite bricks. Geopolymer composite bricks are made by mixing sand, geopolymers synthesized from fly ash with NaOH and Na2SiO3 and calcium oxide calcined from feather clam shell which is printed in cylinder form. The bricks are then cured for 28 days and physical tests are carried out in the form of density, water absorption and porosity tests. The results showed that the most optimal addition of CaO is 7.5% for the physical properties of geopolymer composite bricks with a density value of 1.80 gr/cm3, a porosity value of 10.30% and a water absorption capacity of 4.68%. The value has filled the quality standard 1st for bricks set by Indonesian National Standard (SNI).
从羽蛤壳中添加氧化钙对孔隙率和吸水性土工聚合物复合砖的影响
本研究的目的是研究添加蛤壳灰中的氧化钙(CaO)对土工聚合物复合砖的密度、孔隙率和吸水性等物理性质的影响。土工聚合物复合砖是由沙子、用 NaOH 和 Na2SiO3 与粉煤灰合成的土工聚合物以及从羽毛蚌壳中煅烧出的氧化钙混合制成的。然后将砖块固化 28 天,并进行密度、吸水率和孔隙率等物理测试。结果表明,对于土工聚合物复合砖的物理性能而言,氧化钙的最佳添加量为 7.5%,其密度值为 1.80 gr/cm3,孔隙率值为 10.30%,吸水率为 4.68%。该值符合印尼国家标准(SNI)规定的砖质量标准 1。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信