{"title":"[Electron-probe microanalysis examination of acid-proof dentin layer].","authors":"T Fukushima, Y Inoue, M Kawaguchi, T Horibe","doi":"","DOIUrl":null,"url":null,"abstract":"<p><p>To predict the presence and thickness of the acid-proof dentin layer by the method of combining the halogenated methacrylate and electron-probe microanalyzer (EPMA), 2-methacryloyloxyethyl hydrogen chloromaleate (CIMEM) used as a base monomer for a bonding agent and 2-bromoethyl methacrylate (2 BEM), 2-(4-bromophenyl)ethyl methacrylate (BPy1EM), 2-(4-bromo-1-naphthyl)ethyl methacrylate (BNEM) and 2,4,6-tribromophenoxy methacrylate (TriBr-PM) used as tracers were synthesized. The bond strength to dentin treated with 37% phosphoric acid solution for 30 sec. was not statistically different for the bonding agents with and without tracers. The SEM micrographs revealed that the layers, which may be acid-proof dentin layers, were 3-4 microns thick at the resin-dentin interface for all bonding agents. According to EPMA analysis, cps of C1Ka and BrLa increase at the same points and the acid-proof dentin layer thickness was about 4 microns.</p>","PeriodicalId":77622,"journal":{"name":"Shika zairyo, kikai = Journal of the Japanese Society for Dental Materials and Devices","volume":"9 3","pages":"482-6"},"PeriodicalIF":0.0000,"publicationDate":"1990-05-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Shika zairyo, kikai = Journal of the Japanese Society for Dental Materials and Devices","FirstCategoryId":"1085","ListUrlMain":"","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
To predict the presence and thickness of the acid-proof dentin layer by the method of combining the halogenated methacrylate and electron-probe microanalyzer (EPMA), 2-methacryloyloxyethyl hydrogen chloromaleate (CIMEM) used as a base monomer for a bonding agent and 2-bromoethyl methacrylate (2 BEM), 2-(4-bromophenyl)ethyl methacrylate (BPy1EM), 2-(4-bromo-1-naphthyl)ethyl methacrylate (BNEM) and 2,4,6-tribromophenoxy methacrylate (TriBr-PM) used as tracers were synthesized. The bond strength to dentin treated with 37% phosphoric acid solution for 30 sec. was not statistically different for the bonding agents with and without tracers. The SEM micrographs revealed that the layers, which may be acid-proof dentin layers, were 3-4 microns thick at the resin-dentin interface for all bonding agents. According to EPMA analysis, cps of C1Ka and BrLa increase at the same points and the acid-proof dentin layer thickness was about 4 microns.