{"title":"THE EFFECT OF DIFFERENT LIGHT CURED UNIT INTENSITIES ON THE DEPTH OF POLYMERIZATION OF BULK FILL SCULPTABLE COMPOSITE RESIN RESTORATIONS","authors":"Alphania Esty Luthfaida, Arlina Nurhapsari, H. Fathurrahman","doi":"10.30659/medali.v3i1.16382","DOIUrl":null,"url":null,"abstract":"Background : The latest development of dental material restoration is a bulk fill sculptable composite resin. This material can be applied to a 4 mm cavity at once irradiation. The success of polymerization can be affected by improper irradiation. Both the physical and mechanical properties of the material also can be decreased by improper irradiation. This study aimed to determine the effect of different light-cured unit intensities on the depth of polymerization of bulk fills sculptable composite resin restorations.Method : This research method was an experimental analytic type of post-test only control group design laboratory, consisting of 24 bulk fill sculptable composite resin with a diameter of 4mm x 6mm thickness divided into 6 groups:A1(3M ESPE-low intensity),A2(3M ESPE-high intensity),A3(3M ESPE-soft start intensity),B1(Ivoclar vivacity-low intensity),B2(Ivoclar vivadent-high intensity) and B3(Ivoclar vivadent-soft start intensity). Result : The results showed a significant effect of the low, high, and soft start intensity light-cured units in the bulk fill sculptable composite resin groups by Kruskal-Wallis test 0.00 (p <0.05).Conclusion : The best polymerization depth of bulk fill sculptable composite resin was 3M ESPE and it was affected by the high and low-intensity light-cured units","PeriodicalId":156596,"journal":{"name":"Jurnal Medali","volume":"1 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2021-09-28","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Jurnal Medali","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.30659/medali.v3i1.16382","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

Background : The latest development of dental material restoration is a bulk fill sculptable composite resin. This material can be applied to a 4 mm cavity at once irradiation. The success of polymerization can be affected by improper irradiation. Both the physical and mechanical properties of the material also can be decreased by improper irradiation. This study aimed to determine the effect of different light-cured unit intensities on the depth of polymerization of bulk fills sculptable composite resin restorations.Method : This research method was an experimental analytic type of post-test only control group design laboratory, consisting of 24 bulk fill sculptable composite resin with a diameter of 4mm x 6mm thickness divided into 6 groups:A1(3M ESPE-low intensity),A2(3M ESPE-high intensity),A3(3M ESPE-soft start intensity),B1(Ivoclar vivacity-low intensity),B2(Ivoclar vivadent-high intensity) and B3(Ivoclar vivadent-soft start intensity). Result : The results showed a significant effect of the low, high, and soft start intensity light-cured units in the bulk fill sculptable composite resin groups by Kruskal-Wallis test 0.00 (p <0.05).Conclusion : The best polymerization depth of bulk fill sculptable composite resin was 3M ESPE and it was affected by the high and low-intensity light-cured units
不同光固化单元强度对体填充可塑复合树脂修复体聚合深度的影响
背景:口腔修复材料的最新发展是可塑复合树脂填充体。这种材料可以一次照射到一个4毫米的腔内。不适当的辐照会影响聚合的成功。不适当的辐照也会降低材料的物理和机械性能。本研究旨在确定不同光固化单元强度对大块填充可塑复合树脂修复体聚合深度的影响。方法:本研究方法为实验分析型试验后仅对照组设计实验室,由24块直径为4mm × 6mm厚度的散装填充可塑复合树脂组成,分为6组:A1(3M espe -低强度)、A2(3M espe -高强度)、A3(3M espe -软启动强度)、B1(ivivar -低强度)、B2(ivivar -高强度)和B3(ivivar -软启动强度)。结果:经Kruskal-Wallis检验,低、高、软启动强度光固化单元对大填充可塑复合树脂组有显著影响(p <0.05)。结论:体积填充型可塑复合树脂的最佳聚合深度为3M ESPE,受光固化单元高低强度的影响
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:604180095
Book学术官方微信