{"title":"Marginal Accuracy of Fully Contoured Zirconia Veneer With Two Preparation Designs","authors":"Hend Elkawash, Moamen Ahmed Abd Elkader","doi":"10.21608/aadj.2019.60177","DOIUrl":null,"url":null,"abstract":"ABSTRACT Aim: The purpose of this study is to evaluate the marginal accuracy of fully contoured zirconia laminate veneer utilizing two preparation designs; butt joint incisal reduction and incisal chamfer with palatal over lab. Subjects and Methods: fortyeight maxillary central incisors were prepared into two designs in relation to incisal finish line of laminate preparation; butt joint incisal reduction and incisal chamfer with palatal over lab. Half of samples were restored with pressable lithium disilicate (e.max) as control group, and the other half were restored with fully contoured translucent machinable zirconia (Bruxzair). All laminates were cemented with resin cement and the marginal accuracy were measured. Results: With butt-joint margin design; it was found that e.max group recorded statistically significant higher marginal gap mean value (63.54±1.8 µm) than translucent Zirconia group (57.19±8.4 µm) as indicated by unpaired t-test (t value=2.6, P=0.0179<0.05) .With over-lap margin design; it was found that e.max group recorded statistically significant higher marginal gap mean value (73.46±11.2 µm) than translucent Zirconia group (64.58±5.1 µm) as indicated by unpaired t-test (t value=2.5, P=0.0203 < 0.05). Conclusion:  The marginal accuracy of the fully contoured zirconia veneer showed high adaptation supporting its usage for laminate veneer fabrication.","PeriodicalId":136230,"journal":{"name":"Al-Azhar Assiut Dental Journal","volume":"27 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2019-04-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Al-Azhar Assiut Dental Journal","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.21608/aadj.2019.60177","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

ABSTRACT Aim: The purpose of this study is to evaluate the marginal accuracy of fully contoured zirconia laminate veneer utilizing two preparation designs; butt joint incisal reduction and incisal chamfer with palatal over lab. Subjects and Methods: fortyeight maxillary central incisors were prepared into two designs in relation to incisal finish line of laminate preparation; butt joint incisal reduction and incisal chamfer with palatal over lab. Half of samples were restored with pressable lithium disilicate (e.max) as control group, and the other half were restored with fully contoured translucent machinable zirconia (Bruxzair). All laminates were cemented with resin cement and the marginal accuracy were measured. Results: With butt-joint margin design; it was found that e.max group recorded statistically significant higher marginal gap mean value (63.54±1.8 µm) than translucent Zirconia group (57.19±8.4 µm) as indicated by unpaired t-test (t value=2.6, P=0.0179<0.05) .With over-lap margin design; it was found that e.max group recorded statistically significant higher marginal gap mean value (73.46±11.2 µm) than translucent Zirconia group (64.58±5.1 µm) as indicated by unpaired t-test (t value=2.5, P=0.0203 < 0.05). Conclusion:  The marginal accuracy of the fully contoured zirconia veneer showed high adaptation supporting its usage for laminate veneer fabrication.
两种制备设计的全轮廓氧化锆单板边缘精度
摘要目的:本研究的目的是评估采用两种制备设计的全轮廓氧化锆层压板贴面的边缘精度;对接切复位和切角与腭在实验室。对象与方法:48个上颌中切牙按照层压预备的终点线分为两种设计;对接切复位和切角与腭在实验室。一半的样品用可压二硅酸锂(e.max)修复作为对照组,另一半样品用完全轮廓的半透明可加工氧化锆(Bruxzair)修复。所有层压板都用树脂水泥胶结,并测量边缘精度。结果:采用对接缘设计;未配对t检验(t值=2.6,P=0.0179<0.05)发现,e.max组的边缘间隙平均值(63.54±1.8µm)高于半透明氧化锆组(57.19±8.4µm),差异有统计学意义。未经配对t检验(t值=2.5,P=0.0203 < 0.05), e.max组的边缘间隙平均值(73.46±11.2µm)高于半透明Zirconia组(64.58±5.1µm),具有统计学意义。结论:全轮廓氧化锆贴面的边缘精度具有较高的适应性,可用于复合贴面制作。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:604180095
Book学术官方微信