{"title":"Development of a Hybrid Method for Identifying the Causes of Product Incompatibility in Metallurgical Manufacturing","authors":"R. Dwornicka","doi":"10.21741/9781644902691-24","DOIUrl":null,"url":null,"abstract":"Abstract. For the analysis of the quality of metallurgical products, it is important to use techniques that identify the internal and external unconformity of the product without destroying it. These techniques are non-destructive testing (NDT). Although these techniques identify the unconformity of the product, they do not indicate the source of their creation. The purpose of the study was to develop a hybrid method to make decisions about the causes of product incompatibility. This hybrid method was created as a combination of NDT and quality management techniques, i.e.: 5W2H method, Ishikawa diagram, 5Why method. The subject of the study was an unconformity detected in the tube made of the magnesium alloy AMS 4439. Research was carried out using the FPI method. In the analyzed case, its application allowed the detection of a linear indication in the product. To identify the root of the linear indication, the 5W2H method, the Ishikawa diagram, and the 5Why method were used sequentially. The main causes were bad casting and pollution. The root cause was defective supplier material. Integration of the FPI method, the 5W2H method, the Ishikawa diagram, and the 5Why method in the performance of a comprehensive qualitative analyze of products, after which it is possible to identify the unconformity and the root of its occurrence. The integration of FPI and quality management techniques can be practiced to analyze the quality of products (including metallurgical products) in manufacturing and service enterprises.","PeriodicalId":106609,"journal":{"name":"Quality Production Improvement and System Safety","volume":"1 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2023-09-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Quality Production Improvement and System Safety","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.21741/9781644902691-24","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

Abstract. For the analysis of the quality of metallurgical products, it is important to use techniques that identify the internal and external unconformity of the product without destroying it. These techniques are non-destructive testing (NDT). Although these techniques identify the unconformity of the product, they do not indicate the source of their creation. The purpose of the study was to develop a hybrid method to make decisions about the causes of product incompatibility. This hybrid method was created as a combination of NDT and quality management techniques, i.e.: 5W2H method, Ishikawa diagram, 5Why method. The subject of the study was an unconformity detected in the tube made of the magnesium alloy AMS 4439. Research was carried out using the FPI method. In the analyzed case, its application allowed the detection of a linear indication in the product. To identify the root of the linear indication, the 5W2H method, the Ishikawa diagram, and the 5Why method were used sequentially. The main causes were bad casting and pollution. The root cause was defective supplier material. Integration of the FPI method, the 5W2H method, the Ishikawa diagram, and the 5Why method in the performance of a comprehensive qualitative analyze of products, after which it is possible to identify the unconformity and the root of its occurrence. The integration of FPI and quality management techniques can be practiced to analyze the quality of products (including metallurgical products) in manufacturing and service enterprises.
冶金制造中产品不相容原因识别的混合方法的发展
摘要对于冶金产品的质量分析,重要的是使用技术来识别产品的内部和外部不符合,而不破坏它。这些技术就是无损检测(NDT)。虽然这些技术识别了产品的不符合,但它们并没有指明其产生的来源。本研究的目的是开发一种混合方法来决定产品不相容的原因。这种混合方法是无损检测和质量管理技术的结合,即:5W2H法,Ishikawa图,5Why法。该研究的对象是在镁合金AMS 4439制成的管子中检测到的不合格。采用FPI方法进行了研究。在分析的情况下,其应用允许在产品中检测线性指示。为了确定线性指示的根源,依次使用了5W2H法、石川图法和5Why法。主要原因是铸造不良和污染。根本原因是有缺陷的供应商材料。整合FPI法、5W2H法、石川图、5Why法对产品的性能进行全面的定性分析,识别不合格及其发生的根源。可将FPI与质量管理技术相结合,对制造和服务企业的产品(包括冶金产品)进行质量分析。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信