{"title":"[Examination of shear strength of repaired composite specimen].","authors":"H G Schaller, W Götze, M Siedler","doi":"","DOIUrl":null,"url":null,"abstract":"<p><p>The test of the shearstrength of two composite-inlay-materials and two posterior composites exhibited a statistically significant less bond-strength of repaired specimen compaired with unrepaired control-groups, whereas each material showed different results. The indirect-inlay-system proved to have the lowest bondstrength after repairing. The combination of the two posterior composites as well as the two inlay-systems with each other showed that none of these materials was convincing as a repairing material.</p>","PeriodicalId":77521,"journal":{"name":"Deutsche Stomatologie (Berlin, Germany : 1990)","volume":"41 5","pages":"149-52"},"PeriodicalIF":0.0000,"publicationDate":"1991-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Deutsche Stomatologie (Berlin, Germany : 1990)","FirstCategoryId":"1085","ListUrlMain":"","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
The test of the shearstrength of two composite-inlay-materials and two posterior composites exhibited a statistically significant less bond-strength of repaired specimen compaired with unrepaired control-groups, whereas each material showed different results. The indirect-inlay-system proved to have the lowest bondstrength after repairing. The combination of the two posterior composites as well as the two inlay-systems with each other showed that none of these materials was convincing as a repairing material.