{"title":"Effect of current pulse duration on the thickness and roughness of electrospark coatings","authors":"R. Saifullin, R. Galiullin, L. Islamov","doi":"10.36652/1813-1336-2022-18-3-129-131","DOIUrl":null,"url":null,"abstract":"The effect of the current pulse time on the roughness and surface continuity of the electrospark coating is studied. It is established that in the coating mode: the current pulse time is 2•10–5 s, the frequency is 250 Hz, the stress is 50 V, the roughness parameter is Rz = 80 µm, the continuity is high, but the disadvantage is the low productivity of the process.","PeriodicalId":178558,"journal":{"name":"Strengthening Technologies and Coatings","volume":"46 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"1900-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Strengthening Technologies and Coatings","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.36652/1813-1336-2022-18-3-129-131","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
The effect of the current pulse time on the roughness and surface continuity of the electrospark coating is studied. It is established that in the coating mode: the current pulse time is 2•10–5 s, the frequency is 250 Hz, the stress is 50 V, the roughness parameter is Rz = 80 µm, the continuity is high, but the disadvantage is the low productivity of the process.