{"title":"Ekstrak Daun Jambu Bol (Syzygium Malaccense) sebagai Inhibitor Korosi pada Kawat Ortodontik","authors":"M. F. Zulkaham, Dahyunir Dahlan","doi":"10.25077/jfu.12.2.322-327.2023","DOIUrl":null,"url":null,"abstract":"of the maximum corrosion rate and inhibition efficiency was in samples with a concentration of 10 g/L and 48 hours of immersion time, which was 1.19 mils per year (mpy), and the inhibition efficiency was 91.71%. Morphology to observe the surface using an optical microscope and determine the formed phase using X-Ray Diffraction (XRD). The longer the immersion of the sample with the inhibitor, the better the adsorbed inhibitor and the lower the corrosion rate. An increasing concentration will result in a smaller corrosion rate if the inhibitor concentration is given correctly.","PeriodicalId":221594,"journal":{"name":"Jurnal Fisika Unand","volume":"14 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2023-04-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Jurnal Fisika Unand","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.25077/jfu.12.2.322-327.2023","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
of the maximum corrosion rate and inhibition efficiency was in samples with a concentration of 10 g/L and 48 hours of immersion time, which was 1.19 mils per year (mpy), and the inhibition efficiency was 91.71%. Morphology to observe the surface using an optical microscope and determine the formed phase using X-Ray Diffraction (XRD). The longer the immersion of the sample with the inhibitor, the better the adsorbed inhibitor and the lower the corrosion rate. An increasing concentration will result in a smaller corrosion rate if the inhibitor concentration is given correctly.