{"title":"Surface degradation of glass measured by nanoindentation","authors":"T. Sawa, K. Tanaka","doi":"10.1080/01418610208235728","DOIUrl":null,"url":null,"abstract":"Abstract Nanoindentation tests at the maximum loads P max = 50 and 10 μN were conducted to examine the surface degradation of two glasses: alkaline-earth aluminosilicate as-fused glass for a liquid-crystal substrate and mechanically polished optical lead F-1 glass. The load P-penetration depth h curve for the substrate glass followed an ideal square power law, while that for the F-1 glass deviated from the square power law at the initial stage up to h = 6.0nm. X-ray photoelectron spectroscopy revealed that O—H bonds were formed on the surface of the F-1 glass, suggesting the occurrence of degradation, while no O—H peak was detected on the surface of substrate glass.","PeriodicalId":114492,"journal":{"name":"Philosophical Magazine A","volume":"46 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2002-07-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Philosophical Magazine A","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1080/01418610208235728","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
Abstract Nanoindentation tests at the maximum loads P max = 50 and 10 μN were conducted to examine the surface degradation of two glasses: alkaline-earth aluminosilicate as-fused glass for a liquid-crystal substrate and mechanically polished optical lead F-1 glass. The load P-penetration depth h curve for the substrate glass followed an ideal square power law, while that for the F-1 glass deviated from the square power law at the initial stage up to h = 6.0nm. X-ray photoelectron spectroscopy revealed that O—H bonds were formed on the surface of the F-1 glass, suggesting the occurrence of degradation, while no O—H peak was detected on the surface of substrate glass.