ANALYZE ON VARIATION COMPOSITION OF COMPOSITE POLYMER FOAM POLYURETHANE REINFORCED BY BAGASSE WASTE DUE TO STATIC COMPRESSIVE LOADING

Aidi Sutikno, Taufan Arif Adlie, Zainal Arif
{"title":"ANALYZE ON VARIATION COMPOSITION OF COMPOSITE POLYMER FOAM POLYURETHANE REINFORCED BY BAGASSE WASTE DUE TO STATIC COMPRESSIVE LOADING","authors":"Aidi Sutikno, Taufan Arif Adlie, Zainal Arif","doi":"10.55377/jurutera.v9i01.6743","DOIUrl":null,"url":null,"abstract":"At this time, the discovery in the field of composites continues to grow. Using foamed polymer composites reinforced with natural fibers continues to be researched and developed to obtain alternative materials to replace metals. Composite materials have unique characteristics and are lighter in weight. Natural fibers from bagasse fiber can function as reinforcement in polymer composites. This study aimed to obtain the effect of variations in bagasse fiber on composite polymer foam materials due to compressive strength loads. This polymer composite material was made by varying bagasse fiber with a mesh fiber size of 300, 400, and 500. Three variations of the constituent materials were measured based on the density ratio of the materials. The constituent materials consist of resin, polyurethane, and fiber, respectively are: label A = (85%, 15%, 0%); label B = (84%, 15%, 1%); Label C = (83%,15%, 2%); and label D = (82%, 15%, 3%). Specimens, for each composition, are three specimens. The technique for making specimens uses the method of pouring into molds concerning ASTM D-638. The testing machine for compressive strength of this polymer composite material using the Tensilon RTF-1350 tool. From the data obtained from the results of the maximum compressive strength test occurs in the fiber size of the specimen labeled D (500 Mesh) with a compressive stress of 5.674 MPa and a strain of 0.186 mm/mm. From these data, it can be concluded that the smaller the size of the bagasse fiber, the better the tensile strength of the polymer foam composite material.","PeriodicalId":414829,"journal":{"name":"JURUTERA - Jurnal Umum Teknik Terapan","volume":"58 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2022-12-03","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"JURUTERA - Jurnal Umum Teknik Terapan","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.55377/jurutera.v9i01.6743","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

At this time, the discovery in the field of composites continues to grow. Using foamed polymer composites reinforced with natural fibers continues to be researched and developed to obtain alternative materials to replace metals. Composite materials have unique characteristics and are lighter in weight. Natural fibers from bagasse fiber can function as reinforcement in polymer composites. This study aimed to obtain the effect of variations in bagasse fiber on composite polymer foam materials due to compressive strength loads. This polymer composite material was made by varying bagasse fiber with a mesh fiber size of 300, 400, and 500. Three variations of the constituent materials were measured based on the density ratio of the materials. The constituent materials consist of resin, polyurethane, and fiber, respectively are: label A = (85%, 15%, 0%); label B = (84%, 15%, 1%); Label C = (83%,15%, 2%); and label D = (82%, 15%, 3%). Specimens, for each composition, are three specimens. The technique for making specimens uses the method of pouring into molds concerning ASTM D-638. The testing machine for compressive strength of this polymer composite material using the Tensilon RTF-1350 tool. From the data obtained from the results of the maximum compressive strength test occurs in the fiber size of the specimen labeled D (500 Mesh) with a compressive stress of 5.674 MPa and a strain of 0.186 mm/mm. From these data, it can be concluded that the smaller the size of the bagasse fiber, the better the tensile strength of the polymer foam composite material.
甘蔗渣增强复合聚合物泡沫聚氨酯在静压缩载荷作用下的组分变化分析
此时,在复合材料领域的发现不断增长。利用天然纤维增强的泡沫聚合物复合材料不断被研究和开发,以获得替代金属的替代材料。复合材料具有独特的特性,重量更轻。甘蔗渣纤维中提取的天然纤维可作为高分子复合材料的增强材料。本研究旨在了解甘蔗渣纤维含量的变化对复合聚合物泡沫材料抗压强度载荷的影响。这种聚合物复合材料是由不同的甘蔗渣纤维制成的,网状纤维的尺寸为300、400和500。根据材料的密度比,测量了组成材料的三种变化。组成材料为树脂、聚氨酯、纤维,标签A = (85%, 15%, 0%);标签B = (84%, 15%, 1%);标签C = (83%,15%, 2%);标签D =(82%, 15%, 3%)。每种成分的标本为三个标本。制作样品的技术采用ASTM D-638规定的浇筑模具的方法。使用Tensilon RTF-1350工具测试这种聚合物复合材料的抗压强度。从最大抗压强度试验结果得到的数据来看,发生在纤维尺寸为D(500目)的试样中,其抗压应力为5.674 MPa,应变为0.186 mm/mm。从这些数据可以得出结论,蔗渣纤维的粒径越小,聚合物泡沫复合材料的抗拉强度越好。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信