Utilization of Waste Glass as Filler Material for Concrete Bricks

Riska Iga Saputri, Y. Tethool, R. O. Pramanagara
{"title":"Utilization of Waste Glass as Filler Material for Concrete Bricks","authors":"Riska Iga Saputri, Y. Tethool, R. O. Pramanagara","doi":"10.30862/jistech.v12i1.207","DOIUrl":null,"url":null,"abstract":"Concrete brick is a type of building element in the form of blocks made from the main ingredients of portland cement, water and aggregate used for wall (SNI 03-0349-1989). The concrete brick tested using glass powder added material is expected to produce high compressive strength and low water absorption. The method used is an experimental method by direct research at the Mining Laboratory of the University of Papua and processing the results of compressive strength and water absorption test data.The results of the compressive strength test for concrete bricks with the addition of glass powder with a large compressive strength value, namely in a 10% mixture of 36.256 kg/cm2, when viewed from the quality level based on SNI 03-0349-1989, concrete bricks with the addition of 10% glass powder are included in class IV category.The results of the calculation of water absorption obtained an average value of 0% glass powder, equal to 2.17%, 5% glass powder amounted to 5.08%, and 10% glass powder amounted to 4.92%, when viewed in a quality level based on SNI 03-0349-1989, concrete bricks with the addition of glass powder 0%, 5% and 10% fall into the class I category, namely 25%.The calculation results show that the cost of raw materials for concrete bricks with a mixture of 0% is Rp. 1,130,440, Concrete brick with a 5% mixture of Rp. 1,126,840, Concrete brick with a 10% mixture of Rp. 1,126,240. The results of the calculation of raw material costs show that using glass filler as a substitute for sand in the manufacture of concrete bricks is cheaper than normal concrete bricks.","PeriodicalId":180454,"journal":{"name":"JISTECH: Journal of Information Science and Technology","volume":"22 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2023-06-21","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"JISTECH: Journal of Information Science and Technology","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.30862/jistech.v12i1.207","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

Concrete brick is a type of building element in the form of blocks made from the main ingredients of portland cement, water and aggregate used for wall (SNI 03-0349-1989). The concrete brick tested using glass powder added material is expected to produce high compressive strength and low water absorption. The method used is an experimental method by direct research at the Mining Laboratory of the University of Papua and processing the results of compressive strength and water absorption test data.The results of the compressive strength test for concrete bricks with the addition of glass powder with a large compressive strength value, namely in a 10% mixture of 36.256 kg/cm2, when viewed from the quality level based on SNI 03-0349-1989, concrete bricks with the addition of 10% glass powder are included in class IV category.The results of the calculation of water absorption obtained an average value of 0% glass powder, equal to 2.17%, 5% glass powder amounted to 5.08%, and 10% glass powder amounted to 4.92%, when viewed in a quality level based on SNI 03-0349-1989, concrete bricks with the addition of glass powder 0%, 5% and 10% fall into the class I category, namely 25%.The calculation results show that the cost of raw materials for concrete bricks with a mixture of 0% is Rp. 1,130,440, Concrete brick with a 5% mixture of Rp. 1,126,840, Concrete brick with a 10% mixture of Rp. 1,126,240. The results of the calculation of raw material costs show that using glass filler as a substitute for sand in the manufacture of concrete bricks is cheaper than normal concrete bricks.
废玻璃作为混凝土砖填料的利用
混凝土砖是一种以硅酸盐水泥、水和用于墙体的骨料为主要成分制成的砌块形式的建筑构件(SNI 03-0349-1989)。使用玻璃粉添加料进行的混凝土砖试验有望产生高抗压强度和低吸水率。所使用的方法是由巴布亚大学采矿实验室直接研究并处理抗压强度和吸水试验数据结果的实验方法。抗压强度值较大的玻璃粉掺入混凝土砖的抗压强度试验结果,即在掺量为36.256 kg/cm2的10%混合料中,从SNI 03-0349-1989的质量等级来看,掺量为10%玻璃粉的混凝土砖属于IV类。通过计算得出的吸水率平均值为0%玻璃粉为2.17%,5%玻璃粉为5.08%,10%玻璃粉为4.92%,从SNI 03-0349-1989的质量等级来看,玻璃粉掺量为0%、5%和10%的混凝土砖均为I类,即25%。计算结果表明:掺量为0%的混凝土砖原料成本为1,130,440卢比,掺量为5%的混凝土砖原料成本为1,126,840卢比,掺量为10%的混凝土砖原料成本为1,126,240卢比。原料成本计算结果表明,用玻璃填料代替砂石生产混凝土砖比普通混凝土砖成本低。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:604180095
Book学术官方微信