Guoxiang Peng, Yung-Mao Cheng, Cheng-Fu Yang, Jing Liu, S. Wu, Pei-Ying Lin
{"title":"Investigation of the Optical Characteristics of the Eu2O3-Doped Sr3Al2O6 Phosphors","authors":"Guoxiang Peng, Yung-Mao Cheng, Cheng-Fu Yang, Jing Liu, S. Wu, Pei-Ying Lin","doi":"10.1109/ICIASE45644.2019.9074017","DOIUrl":null,"url":null,"abstract":"In this research, we used the solid-state reaction method to synthesize the Eu<inf>2</inf>O<inf>3</inf>-doped Sr<inf>3</inf>Al<inf>2</inf>O<inf>6</inf> powder with the different temperatures. The Eu<inf>2</inf>O<inf>3</inf>-doped Sr<inf>3</inf>Al<inf>2</inf>O<inf>6</inf> powder was synthesized at 1000°C–1300°C for 4 h. The variations in the morphologies of Eu<inf>2</inf>O<inf>3</inf>-doped Sr<inf>3</inf>Al<inf>2</inf>O<inf>6</inf> phosphors were observed using a FESEM. As the synthesizing temperature increases, the crystallization and particle sizes of the Eu<inf>2</inf>O<inf>3</inf>-doped Sr<inf>3</inf>Al<inf>2</inf>O<inf>6</inf> composition are significantly improved. From the photoluminescence excitation spectrum we found that 240 nm was the optimum excitation optical wavelength to excite the Eu<inf>2</inf>O<inf>3</inf>-doped Sr<inf>3</inf>Al<inf>2</inf>O<inf>6</inf> phosphors. We had also found that the emission (PL) spectra of the Eu<inf>2</inf>O<inf>3</inf>-doped Sr<inf>3</inf>Al<inf>2</inf>O<inf>6</inf> phosphors had sharp peaks in three strong peaks at 389, 592, and 612 nm and had small peak in two weak bands at 290 nm and 651~653 nm.","PeriodicalId":206741,"journal":{"name":"2019 IEEE International Conference of Intelligent Applied Systems on Engineering (ICIASE)","volume":"37 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2019-04-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"2019 IEEE International Conference of Intelligent Applied Systems on Engineering (ICIASE)","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1109/ICIASE45644.2019.9074017","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
In this research, we used the solid-state reaction method to synthesize the Eu2O3-doped Sr3Al2O6 powder with the different temperatures. The Eu2O3-doped Sr3Al2O6 powder was synthesized at 1000°C–1300°C for 4 h. The variations in the morphologies of Eu2O3-doped Sr3Al2O6 phosphors were observed using a FESEM. As the synthesizing temperature increases, the crystallization and particle sizes of the Eu2O3-doped Sr3Al2O6 composition are significantly improved. From the photoluminescence excitation spectrum we found that 240 nm was the optimum excitation optical wavelength to excite the Eu2O3-doped Sr3Al2O6 phosphors. We had also found that the emission (PL) spectra of the Eu2O3-doped Sr3Al2O6 phosphors had sharp peaks in three strong peaks at 389, 592, and 612 nm and had small peak in two weak bands at 290 nm and 651~653 nm.