美容树脂基体和氧化锆增强二硅酸锂 CAD/CAM 材料的磨损特性:双体磨损和表面形貌分析。

IF 1.1 Q3 DENTISTRY, ORAL SURGERY & MEDICINE
Minerva dental and oral science Pub Date : 2023-12-01 Epub Date: 2023-05-31 DOI:10.23736/S2724-6329.23.04779-4
Mohamed M Radwan, Ahmed Abdou, Nermeen Nagi, Dina H Younes, Aliaa Mahrous
{"title":"美容树脂基体和氧化锆增强二硅酸锂 CAD/CAM 材料的磨损特性:双体磨损和表面形貌分析。","authors":"Mohamed M Radwan, Ahmed Abdou, Nermeen Nagi, Dina H Younes, Aliaa Mahrous","doi":"10.23736/S2724-6329.23.04779-4","DOIUrl":null,"url":null,"abstract":"<p><strong>Background: </strong>This in vitro study assessed the wear behavior of different CAD-CAM blocks and the abrasion of the enamel antagonist against these materials.</p><p><strong>Methods: </strong>64 disk-shaped specimens were prepared from 8 different CAD/CAM blocks as follow: one lithium disilicate glass ceramics block \"IPS Emax CAD\" as control group, two zirconia reinforced lithium silicate \"Vita Suprinity & Celtra DUO,\" one interpenetrating network ceramic block \"Vita Enamic,\" Three resin-based block composites \"Lava Ultimate, Cerasmart & Brilliant-crios\" as well as one hybrid nanoceramic \"Shofu block HC\". All specimens were mounted against canine and tested for two body wear analysis using a chewing simulating loading machine (100,000 cycles, 50 N, 5/55 °C). The amount of wear loss was measured for each specimen using a digital precise scale. Wear area before and after the chewing simulation were evaluated using an optical profilometer. Data analysed using one-way ANOVA test followed by Tukey's post hoc.</p><p><strong>Results: </strong>The results showed a significantly higher wear loss in resin matrix ceramics in comparison to glass ceramics. However, for tooth wear glass ceramics had significantly higher value than hybrid ceramics.</p><p><strong>Conclusions: </strong>Resin based CAD/CAM Blocks gives a superior result when evaluating the wear behavior and its effect on the opposing tooth surface.</p>","PeriodicalId":18709,"journal":{"name":"Minerva dental and oral science","volume":null,"pages":null},"PeriodicalIF":1.1000,"publicationDate":"2023-12-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"1","resultStr":"{\"title\":\"Wear characteristics of esthetic resin matrix and zirconia reinforced lithium disilicate CAD/CAM materials: two-body wear and surface topography analysis.\",\"authors\":\"Mohamed M Radwan, Ahmed Abdou, Nermeen Nagi, Dina H Younes, Aliaa Mahrous\",\"doi\":\"10.23736/S2724-6329.23.04779-4\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<p><strong>Background: </strong>This in vitro study assessed the wear behavior of different CAD-CAM blocks and the abrasion of the enamel antagonist against these materials.</p><p><strong>Methods: </strong>64 disk-shaped specimens were prepared from 8 different CAD/CAM blocks as follow: one lithium disilicate glass ceramics block \\\"IPS Emax CAD\\\" as control group, two zirconia reinforced lithium silicate \\\"Vita Suprinity & Celtra DUO,\\\" one interpenetrating network ceramic block \\\"Vita Enamic,\\\" Three resin-based block composites \\\"Lava Ultimate, Cerasmart & Brilliant-crios\\\" as well as one hybrid nanoceramic \\\"Shofu block HC\\\". All specimens were mounted against canine and tested for two body wear analysis using a chewing simulating loading machine (100,000 cycles, 50 N, 5/55 °C). The amount of wear loss was measured for each specimen using a digital precise scale. Wear area before and after the chewing simulation were evaluated using an optical profilometer. Data analysed using one-way ANOVA test followed by Tukey's post hoc.</p><p><strong>Results: </strong>The results showed a significantly higher wear loss in resin matrix ceramics in comparison to glass ceramics. However, for tooth wear glass ceramics had significantly higher value than hybrid ceramics.</p><p><strong>Conclusions: </strong>Resin based CAD/CAM Blocks gives a superior result when evaluating the wear behavior and its effect on the opposing tooth surface.</p>\",\"PeriodicalId\":18709,\"journal\":{\"name\":\"Minerva dental and oral science\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":1.1000,\"publicationDate\":\"2023-12-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"1\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Minerva dental and oral science\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.23736/S2724-6329.23.04779-4\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"2023/5/31 0:00:00\",\"PubModel\":\"Epub\",\"JCR\":\"Q3\",\"JCRName\":\"DENTISTRY, ORAL SURGERY & MEDICINE\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Minerva dental and oral science","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.23736/S2724-6329.23.04779-4","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"2023/5/31 0:00:00","PubModel":"Epub","JCR":"Q3","JCRName":"DENTISTRY, ORAL SURGERY & MEDICINE","Score":null,"Total":0}
引用次数: 1

摘要

背景:这项体外研究评估了不同 CAD-CAM 块体的磨损行为以及釉质拮抗剂对这些材料的磨损情况。方法:从以下 8 种不同的 CAD/CAM 块体中制备出 64 个圆盘状试样:一种二硅酸锂玻璃陶瓷块体 "IPS Emax CAD "作为对照组,两种氧化锆增强硅酸锂 "Vita Suprinity & Celtra DUO",一种互穿网络陶瓷块体 "Vita Enamic",三种树脂基块体复合材料 "Lava Ultimate、Cerasmart & Brilliant-crios "以及一种混合纳米陶瓷 "Shofu block HC"。所有试样都安装在犬齿上,并使用咀嚼模拟加载机(100,000 次循环,50 N,5/55 °C)进行两体磨损分析测试。每个试样的磨损量都是用数字精密刻度尺测量的。使用光学轮廓仪评估模拟咀嚼前后的磨损面积。数据采用单因素方差分析和 Tukey 后验法进行分析:结果表明,与玻璃陶瓷相比,树脂基陶瓷的磨损率明显更高。然而,在牙齿磨损方面,玻璃陶瓷的数值明显高于混合陶瓷:基于树脂的 CAD/CAM 块体在评估磨损行为及其对邻牙表面的影响时效果更佳。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
Wear characteristics of esthetic resin matrix and zirconia reinforced lithium disilicate CAD/CAM materials: two-body wear and surface topography analysis.

Background: This in vitro study assessed the wear behavior of different CAD-CAM blocks and the abrasion of the enamel antagonist against these materials.

Methods: 64 disk-shaped specimens were prepared from 8 different CAD/CAM blocks as follow: one lithium disilicate glass ceramics block "IPS Emax CAD" as control group, two zirconia reinforced lithium silicate "Vita Suprinity & Celtra DUO," one interpenetrating network ceramic block "Vita Enamic," Three resin-based block composites "Lava Ultimate, Cerasmart & Brilliant-crios" as well as one hybrid nanoceramic "Shofu block HC". All specimens were mounted against canine and tested for two body wear analysis using a chewing simulating loading machine (100,000 cycles, 50 N, 5/55 °C). The amount of wear loss was measured for each specimen using a digital precise scale. Wear area before and after the chewing simulation were evaluated using an optical profilometer. Data analysed using one-way ANOVA test followed by Tukey's post hoc.

Results: The results showed a significantly higher wear loss in resin matrix ceramics in comparison to glass ceramics. However, for tooth wear glass ceramics had significantly higher value than hybrid ceramics.

Conclusions: Resin based CAD/CAM Blocks gives a superior result when evaluating the wear behavior and its effect on the opposing tooth surface.

求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
Minerva dental and oral science
Minerva dental and oral science DENTISTRY, ORAL SURGERY & MEDICINE-
CiteScore
2.50
自引率
5.00%
发文量
61
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信