Polyetherimides。2高温溶液聚合

T. Takekoshi, J. E. Kochanowski, J. S. Manello, M. J. Webber
{"title":"Polyetherimides。2高温溶液聚合","authors":"T. Takekoshi,&nbsp;J. E. Kochanowski,&nbsp;J. S. Manello,&nbsp;M. J. Webber","doi":"10.1002/polc.5070740111","DOIUrl":null,"url":null,"abstract":"<p>The polymerization and characterization of the ether-containing aromatic polyimides of the following general structure are presented.</p><p><span>\n <picture>\n <source></source></picture>\n </span></p><p>The polymerization was conducted in one step in homogeneous solution of m-cresol at high temperatures. Typical polyeterimides (PEI) were noncrystalline and showed excellent thermal stability. Among 46 polymers synthesized, only two were crystalline. PEI had glass transition temperatures from 178° to 277°C and exhibited excellent processibility. Many PEI were also soluble in dipolar aprotic solvents and chlorinated hydrocarbons.</p>","PeriodicalId":16867,"journal":{"name":"Journal of Polymer Science: Polymer Symposia","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"1986-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://sci-hub-pdf.com/10.1002/polc.5070740111","citationCount":"58","resultStr":"{\"title\":\"Polyetherimides. II. High-temperature solution polymerization\",\"authors\":\"T. Takekoshi,&nbsp;J. E. Kochanowski,&nbsp;J. S. Manello,&nbsp;M. J. Webber\",\"doi\":\"10.1002/polc.5070740111\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<p>The polymerization and characterization of the ether-containing aromatic polyimides of the following general structure are presented.</p><p><span>\\n <picture>\\n <source></source></picture>\\n </span></p><p>The polymerization was conducted in one step in homogeneous solution of m-cresol at high temperatures. Typical polyeterimides (PEI) were noncrystalline and showed excellent thermal stability. Among 46 polymers synthesized, only two were crystalline. PEI had glass transition temperatures from 178° to 277°C and exhibited excellent processibility. Many PEI were also soluble in dipolar aprotic solvents and chlorinated hydrocarbons.</p>\",\"PeriodicalId\":16867,\"journal\":{\"name\":\"Journal of Polymer Science: Polymer Symposia\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":0.0000,\"publicationDate\":\"1986-01-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"https://sci-hub-pdf.com/10.1002/polc.5070740111\",\"citationCount\":\"58\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Journal of Polymer Science: Polymer Symposia\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://onlinelibrary.wiley.com/doi/10.1002/polc.5070740111\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Polymer Science: Polymer Symposia","FirstCategoryId":"1085","ListUrlMain":"https://onlinelibrary.wiley.com/doi/10.1002/polc.5070740111","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 58

摘要

介绍了以下一般结构的含醚芳族聚酰亚胺的聚合和表征。该聚合反应在间甲酚均相高温下一步完成。典型的聚醚酰亚胺(PEI)是非晶态的,具有良好的热稳定性。在合成的46种聚合物中,只有两种是结晶性的。PEI的玻璃化转变温度为178 ~ 277℃,具有良好的可加工性。许多PEI还可溶于偶极非质子溶剂和氯化烃。
本文章由计算机程序翻译,如有差异,请以英文原文为准。

Polyetherimides. II. High-temperature solution polymerization

Polyetherimides. II. High-temperature solution polymerization

The polymerization and characterization of the ether-containing aromatic polyimides of the following general structure are presented.

The polymerization was conducted in one step in homogeneous solution of m-cresol at high temperatures. Typical polyeterimides (PEI) were noncrystalline and showed excellent thermal stability. Among 46 polymers synthesized, only two were crystalline. PEI had glass transition temperatures from 178° to 277°C and exhibited excellent processibility. Many PEI were also soluble in dipolar aprotic solvents and chlorinated hydrocarbons.

求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信