薄壁球墨铸铁的组织性能相关性

R. Upadhyaya, K. Singh
{"title":"薄壁球墨铸铁的组织性能相关性","authors":"R. Upadhyaya, K. Singh","doi":"10.5539/JMSR.V8N1P1","DOIUrl":null,"url":null,"abstract":"This research work concerns an assessment of the effect of one step inoculation method on thin section castings (2-5) mm analyzed. In this study inoculants representing Ce, Zr and Sr bearing Fe-Si alloys were used. It has been observed that section thickness of 2 mm thin plate containing Ce bearing Fe-Si alloys at 0.4wt% contain mainly pearlitic matrix having microhardness (HV20), ultimate tensile strength (UTS) and percentage of elongation are 272 HV, 720 MPa and 4.5% respectively. It was observed that wear of 2 mm section thickness of thin plate containing Ce bearing Fe-Si alloys have greater wear resistance (272HV) compare to Zr bearing Fe-Si alloys (262HV) and Sr bearing Fe-Si alloys (259HV) respectively at 0.4wt% due to reason of pearlitic and ferritic volume fraction contents present in matrix.","PeriodicalId":16111,"journal":{"name":"Journal of Materials Science Research","volume":"18 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2018-11-14","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Structure Property Correlation of Thin Wall Ductile Iron\",\"authors\":\"R. Upadhyaya, K. Singh\",\"doi\":\"10.5539/JMSR.V8N1P1\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"This research work concerns an assessment of the effect of one step inoculation method on thin section castings (2-5) mm analyzed. In this study inoculants representing Ce, Zr and Sr bearing Fe-Si alloys were used. It has been observed that section thickness of 2 mm thin plate containing Ce bearing Fe-Si alloys at 0.4wt% contain mainly pearlitic matrix having microhardness (HV20), ultimate tensile strength (UTS) and percentage of elongation are 272 HV, 720 MPa and 4.5% respectively. It was observed that wear of 2 mm section thickness of thin plate containing Ce bearing Fe-Si alloys have greater wear resistance (272HV) compare to Zr bearing Fe-Si alloys (262HV) and Sr bearing Fe-Si alloys (259HV) respectively at 0.4wt% due to reason of pearlitic and ferritic volume fraction contents present in matrix.\",\"PeriodicalId\":16111,\"journal\":{\"name\":\"Journal of Materials Science Research\",\"volume\":\"18 1\",\"pages\":\"\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2018-11-14\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Journal of Materials Science Research\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.5539/JMSR.V8N1P1\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Materials Science Research","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.5539/JMSR.V8N1P1","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

研究了一步孕育法对2 ~ 5 mm薄壁铸件的影响。本研究采用了含Ce、Zr和Sr的Fe-Si合金作为孕育剂。结果表明,含Ce铁硅合金厚度为0.4wt%的2 mm薄板断面厚度主要为珠光体基体,显微硬度(HV20)、极限抗拉强度(UTS)和延伸率分别为272 HV、720 MPa和4.5%。结果表明,由于基体中珠光体和铁素体体积分数的存在,含Ce的Fe-Si合金在2 mm截面厚度的薄板上的耐磨性(272HV)比含Zr的Fe-Si合金(262HV)和含Sr的Fe-Si合金(259HV)分别提高了0.4wt%。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
Structure Property Correlation of Thin Wall Ductile Iron
This research work concerns an assessment of the effect of one step inoculation method on thin section castings (2-5) mm analyzed. In this study inoculants representing Ce, Zr and Sr bearing Fe-Si alloys were used. It has been observed that section thickness of 2 mm thin plate containing Ce bearing Fe-Si alloys at 0.4wt% contain mainly pearlitic matrix having microhardness (HV20), ultimate tensile strength (UTS) and percentage of elongation are 272 HV, 720 MPa and 4.5% respectively. It was observed that wear of 2 mm section thickness of thin plate containing Ce bearing Fe-Si alloys have greater wear resistance (272HV) compare to Zr bearing Fe-Si alloys (262HV) and Sr bearing Fe-Si alloys (259HV) respectively at 0.4wt% due to reason of pearlitic and ferritic volume fraction contents present in matrix.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信