{"title":"未掺杂和掺碳钼酸钙催化剂光催化降解孔雀石绿","authors":"Chawda Hardeep Shre, J. Bhatt, Rajendra Singh Rathore, C. Suresh, R. Ameta","doi":"10.30799/JACS.237.21070202","DOIUrl":null,"url":null,"abstract":"Calcium molybdates (undoped and carbon-doped) have been used as a photocatalyst for the degradation of malachite green. These have been characterized by different techniques such as FE-SEM, EDX and XRD. The progress of the reaction has been monitored spectrophotometrically. Different rate affecting parameters like pH, concentration of dye, amount of semiconductor and light intensity have been studied and their optimum values obtained are pH 9.7, concentration of malachite green as 5.00 × 10-4 M, 0.12 g of CaMoO4 and light intensity as 50.0 mWcm–2. A tentative mechanism for the photocatalytic degradation of dye has been proposed, where hydroxyl radical has been observed as an active oxidizing species.","PeriodicalId":14902,"journal":{"name":"Journal of Advanced Chemical Sciences","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"2021-05-26","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"2","resultStr":"{\"title\":\"Photocatalytic Degradation of Malachite Green using Undoped and Carbon-Doped Calcium Molybdate Catalysts\",\"authors\":\"Chawda Hardeep Shre, J. Bhatt, Rajendra Singh Rathore, C. Suresh, R. Ameta\",\"doi\":\"10.30799/JACS.237.21070202\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Calcium molybdates (undoped and carbon-doped) have been used as a photocatalyst for the degradation of malachite green. These have been characterized by different techniques such as FE-SEM, EDX and XRD. The progress of the reaction has been monitored spectrophotometrically. Different rate affecting parameters like pH, concentration of dye, amount of semiconductor and light intensity have been studied and their optimum values obtained are pH 9.7, concentration of malachite green as 5.00 × 10-4 M, 0.12 g of CaMoO4 and light intensity as 50.0 mWcm–2. A tentative mechanism for the photocatalytic degradation of dye has been proposed, where hydroxyl radical has been observed as an active oxidizing species.\",\"PeriodicalId\":14902,\"journal\":{\"name\":\"Journal of Advanced Chemical Sciences\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2021-05-26\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"2\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Journal of Advanced Chemical Sciences\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.30799/JACS.237.21070202\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Advanced Chemical Sciences","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.30799/JACS.237.21070202","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 2

摘要

用钼酸钙(未掺杂和碳掺杂)作为光催化剂降解孔雀石绿。用FE-SEM、EDX和XRD等技术对其进行了表征。用分光光度法对反应过程进行了监测。研究了pH、染料浓度、半导体用量、光强等不同影响速率的参数,得到了pH 9.7、孔雀石绿浓度5.00 × 10-4 M、CaMoO4 0.12 g、光强50.0 mWcm-2的最优值。提出了一种光催化降解染料的初步机制,其中羟基自由基已被观察到作为一种活性氧化物质。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
Photocatalytic Degradation of Malachite Green using Undoped and Carbon-Doped Calcium Molybdate Catalysts
Calcium molybdates (undoped and carbon-doped) have been used as a photocatalyst for the degradation of malachite green. These have been characterized by different techniques such as FE-SEM, EDX and XRD. The progress of the reaction has been monitored spectrophotometrically. Different rate affecting parameters like pH, concentration of dye, amount of semiconductor and light intensity have been studied and their optimum values obtained are pH 9.7, concentration of malachite green as 5.00 × 10-4 M, 0.12 g of CaMoO4 and light intensity as 50.0 mWcm–2. A tentative mechanism for the photocatalytic degradation of dye has been proposed, where hydroxyl radical has been observed as an active oxidizing species.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信