Y. Yokogawa, T. Murata, H. Yamada, K. Fujii, K. Tone, Y. Okada
{"title":"壳聚糖非刚性磷酸钙水泥的合成及性能研究","authors":"Y. Yokogawa, T. Murata, H. Yamada, K. Fujii, K. Tone, Y. Okada","doi":"10.3363/PRB.31.38","DOIUrl":null,"url":null,"abstract":"Calcium phosphate cement (CPC) has biocompatibility and osteoconductive property, but it has some drawbacks, such as wash-out and rigid and brittle properties. Such drawbacks can be overcome by fast-setting and gelation of the CPC paste. The CPC powder is a mixture of tetracalcium phosphate and dicalcium phosphate dehydrate. A low or medium molecular weight chitosan (lowor med-chitosan) and malic acid solution were used in the liquid phase to develop fast-setting and high work-of-fracture CPC materials. The incorporation of 1.25 2.5 wt% chitosan increased a tripled work-of-fracture to 12.0 kJ/m when not using chitosan. The setting time was 2.8±0.3 min and 5.5±0.5 min when 2.5 wt% lowor med-chitosan was used, respectively. The \"non-rigid” and “fast-setting\" CPC cement was successfully obtained by adding chitosan and malic acid to the liquid phase, and the incorporation of med-chitosan may produce a high work-of-fracture and stable CPC with a desirable setting time. (Received March 31, 2016; Accepted May 2, 2016)","PeriodicalId":20022,"journal":{"name":"Phosphorus Research Bulletin","volume":"12 1","pages":"38-43"},"PeriodicalIF":0.0000,"publicationDate":"2016-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"1","resultStr":"{\"title\":\"SYNTHESIS and PROPERTIES of NON-RIGID CALCIUM PHOSPHATE CEMENT CONTAINING CHITOSAN\",\"authors\":\"Y. Yokogawa, T. Murata, H. Yamada, K. Fujii, K. Tone, Y. Okada\",\"doi\":\"10.3363/PRB.31.38\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Calcium phosphate cement (CPC) has biocompatibility and osteoconductive property, but it has some drawbacks, such as wash-out and rigid and brittle properties. Such drawbacks can be overcome by fast-setting and gelation of the CPC paste. The CPC powder is a mixture of tetracalcium phosphate and dicalcium phosphate dehydrate. A low or medium molecular weight chitosan (lowor med-chitosan) and malic acid solution were used in the liquid phase to develop fast-setting and high work-of-fracture CPC materials. The incorporation of 1.25 2.5 wt% chitosan increased a tripled work-of-fracture to 12.0 kJ/m when not using chitosan. The setting time was 2.8±0.3 min and 5.5±0.5 min when 2.5 wt% lowor med-chitosan was used, respectively. The \\\"non-rigid” and “fast-setting\\\" CPC cement was successfully obtained by adding chitosan and malic acid to the liquid phase, and the incorporation of med-chitosan may produce a high work-of-fracture and stable CPC with a desirable setting time. (Received March 31, 2016; Accepted May 2, 2016)\",\"PeriodicalId\":20022,\"journal\":{\"name\":\"Phosphorus Research Bulletin\",\"volume\":\"12 1\",\"pages\":\"38-43\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2016-01-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"1\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Phosphorus Research Bulletin\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.3363/PRB.31.38\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Phosphorus Research Bulletin","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.3363/PRB.31.38","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 1
摘要
磷酸钙水泥(CPC)具有生物相容性和骨导电性,但也存在冲刷、硬脆等缺点。这些缺点可以通过CPC膏体的快速凝固和凝胶化来克服。CPC粉末是磷酸四钙和脱水磷酸二钙的混合物。采用低分子量或中等分子量的壳聚糖(low - medium -chitosan)和苹果酸溶液作为液相,制备了快速凝固和高压裂作业能力的CPC材料。在不使用壳聚糖的情况下,1.25 - 2.5 wt%的壳聚糖的掺入使压裂功增加了三倍,达到12.0 kJ/m。2.5%低浓度壳聚糖的凝固时间分别为2.8±0.3 min和5.5±0.5 min。通过在液相中加入壳聚糖和苹果酸,成功地获得了“非刚性”和“快凝”CPC水泥,并且中壳聚糖的掺入可以产生高压裂功和稳定的CPC,并且具有理想的凝结时间。(2016年3月31日收稿;2016年5月2日录用)
SYNTHESIS and PROPERTIES of NON-RIGID CALCIUM PHOSPHATE CEMENT CONTAINING CHITOSAN
Calcium phosphate cement (CPC) has biocompatibility and osteoconductive property, but it has some drawbacks, such as wash-out and rigid and brittle properties. Such drawbacks can be overcome by fast-setting and gelation of the CPC paste. The CPC powder is a mixture of tetracalcium phosphate and dicalcium phosphate dehydrate. A low or medium molecular weight chitosan (lowor med-chitosan) and malic acid solution were used in the liquid phase to develop fast-setting and high work-of-fracture CPC materials. The incorporation of 1.25 2.5 wt% chitosan increased a tripled work-of-fracture to 12.0 kJ/m when not using chitosan. The setting time was 2.8±0.3 min and 5.5±0.5 min when 2.5 wt% lowor med-chitosan was used, respectively. The "non-rigid” and “fast-setting" CPC cement was successfully obtained by adding chitosan and malic acid to the liquid phase, and the incorporation of med-chitosan may produce a high work-of-fracture and stable CPC with a desirable setting time. (Received March 31, 2016; Accepted May 2, 2016)