CuO/α-Fe2O3纳米复合材料对甲基橙偶氮染料的合成、表征及降解活性研究

Mohsen Mehdipour Ghazi, M. Ilbeigi, M. Jahangiri
{"title":"CuO/α-Fe2O3纳米复合材料对甲基橙偶氮染料的合成、表征及降解活性研究","authors":"Mohsen Mehdipour Ghazi, M. Ilbeigi, M. Jahangiri","doi":"10.22104/AET.2017.427","DOIUrl":null,"url":null,"abstract":"This study investigated the photo-degradation of methyl orange (MO) as a type of azo dye using a CuO/α-Fe2O3 nanocomposite. A CuO/α-Fe2O3 powder with a crystalline size in the range of 27-49 nm was successfully prepared using simple co-precipitation along with a sonication method. The characterization of the synthesized sample was done via XRD, FE-SEM, EDS, FTIR and DRS analyses. The Tauc equation revealed that the band gap of the nano composite in the direct mood was 2.05 ev, which is in the visible light range. The effect of operating factors containing dye concentration, photocatalyst dosage and pH on dye degradation efficiency was measured. Response Surface Method (RSM) was employed to specify the parameter effects. The photocatalytic activity of the CuO/α-Fe2O3 nanocomposite was evaluated by degradation of MO under visible light irradiation. The results showed that the pH value played a very effective role in the dye degradation process efficiency. Also, the photocatalytic degradation of MO obtained was equal to 88.47% in the optimal values.","PeriodicalId":7295,"journal":{"name":"Advances in environmental science and technology","volume":"39 1","pages":"143-151"},"PeriodicalIF":0.0000,"publicationDate":"2017-04-22","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"8","resultStr":"{\"title\":\"Synthesis, characterization and degradation activity of Methyl orange Azo dye using synthesized CuO/α-Fe2O3 nanocomposite\",\"authors\":\"Mohsen Mehdipour Ghazi, M. Ilbeigi, M. Jahangiri\",\"doi\":\"10.22104/AET.2017.427\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"This study investigated the photo-degradation of methyl orange (MO) as a type of azo dye using a CuO/α-Fe2O3 nanocomposite. A CuO/α-Fe2O3 powder with a crystalline size in the range of 27-49 nm was successfully prepared using simple co-precipitation along with a sonication method. The characterization of the synthesized sample was done via XRD, FE-SEM, EDS, FTIR and DRS analyses. The Tauc equation revealed that the band gap of the nano composite in the direct mood was 2.05 ev, which is in the visible light range. The effect of operating factors containing dye concentration, photocatalyst dosage and pH on dye degradation efficiency was measured. Response Surface Method (RSM) was employed to specify the parameter effects. The photocatalytic activity of the CuO/α-Fe2O3 nanocomposite was evaluated by degradation of MO under visible light irradiation. The results showed that the pH value played a very effective role in the dye degradation process efficiency. Also, the photocatalytic degradation of MO obtained was equal to 88.47% in the optimal values.\",\"PeriodicalId\":7295,\"journal\":{\"name\":\"Advances in environmental science and technology\",\"volume\":\"39 1\",\"pages\":\"143-151\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2017-04-22\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"8\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Advances in environmental science and technology\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.22104/AET.2017.427\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Advances in environmental science and technology","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.22104/AET.2017.427","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 8

摘要

本文研究了CuO/α-Fe2O3纳米复合材料对偶氮染料甲基橙(MO)的光降解。采用简单共沉淀法和超声法制备了晶粒尺寸为27 ~ 49 nm的CuO/α-Fe2O3粉体。通过XRD、FE-SEM、EDS、FTIR和DRS对合成样品进行了表征。Tauc方程表明,纳米复合材料在直接情绪下的带隙为2.05 ev,在可见光范围内。考察了含染料浓度、光催化剂用量和pH对染料降解效率的影响。采用响应面法(RSM)表征参数效应。通过可见光下对MO的降解,评价了CuO/α-Fe2O3纳米复合材料的光催化活性。结果表明,pH值对染料降解工艺效率起着非常有效的作用。得到的MO光催化降解率为最优值的88.47%。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
Synthesis, characterization and degradation activity of Methyl orange Azo dye using synthesized CuO/α-Fe2O3 nanocomposite
This study investigated the photo-degradation of methyl orange (MO) as a type of azo dye using a CuO/α-Fe2O3 nanocomposite. A CuO/α-Fe2O3 powder with a crystalline size in the range of 27-49 nm was successfully prepared using simple co-precipitation along with a sonication method. The characterization of the synthesized sample was done via XRD, FE-SEM, EDS, FTIR and DRS analyses. The Tauc equation revealed that the band gap of the nano composite in the direct mood was 2.05 ev, which is in the visible light range. The effect of operating factors containing dye concentration, photocatalyst dosage and pH on dye degradation efficiency was measured. Response Surface Method (RSM) was employed to specify the parameter effects. The photocatalytic activity of the CuO/α-Fe2O3 nanocomposite was evaluated by degradation of MO under visible light irradiation. The results showed that the pH value played a very effective role in the dye degradation process efficiency. Also, the photocatalytic degradation of MO obtained was equal to 88.47% in the optimal values.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信