分析塑料废物替换效果的影响,作为强力冲击混凝土的骨料

Muhamad iqbal Saputra, A. Nasrullah
{"title":"分析塑料废物替换效果的影响,作为强力冲击混凝土的骨料","authors":"Muhamad iqbal Saputra, A. Nasrullah","doi":"10.36050/berings.v6i02.194","DOIUrl":null,"url":null,"abstract":"In general, concrete is composed of cement, fine aggregate, coarse aggregate, water and additional substances if needed. But along with the development of science and technology, concrete constituent materials can also change or be combined with organic or inorganic materials such as plastic waste materials and others. HDPE Plastic (High-Density Polyethylene) Is a type of plastic that is usually used to make milk bottles, detergent bottles, shampoo bottles, moisturizing bottles, oil bottles with code No. 2., toys, and some plastic bags. PET (Polyethylene Terephthalate) PETE or PET is one of the plastics used for food containers, bottles of mineral water and several other wrappers. This plastic is designed for one-time use only. With the use of HDPE and PET plastic waste at a percentage of 20% for concrete compressive strength was not achieved, normal concrete = 15.88 concrete B.HDPE = 12.01, B.PET = 11.71, BC = 12.39 but for concrete weight decreasing, normal concrete = 2330 kg, m3 B.HDPE concrete = 2122 kg, m3, B.PET = 2128 kg, m3, BC = 2096 kg, m3. For the composition of the optimum concrete mixture of the three compositions (B.HDPE, B.PET, BC) obtained the composition of BC which has the most optimum value of 12.39 Mpa, but does not reach the compressive strength of the plan of 15 Mpa.","PeriodicalId":17796,"journal":{"name":"JURNAL ILMIAH BERING'S","volume":"2 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2019-10-07","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"ANALISA PENGARUH SUBSTITUSI LIMBAH PLASTIK SEBAGAI AGREGAT KASAR TERHADAP KUAT TEKAN BETON\",\"authors\":\"Muhamad iqbal Saputra, A. Nasrullah\",\"doi\":\"10.36050/berings.v6i02.194\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"In general, concrete is composed of cement, fine aggregate, coarse aggregate, water and additional substances if needed. But along with the development of science and technology, concrete constituent materials can also change or be combined with organic or inorganic materials such as plastic waste materials and others. HDPE Plastic (High-Density Polyethylene) Is a type of plastic that is usually used to make milk bottles, detergent bottles, shampoo bottles, moisturizing bottles, oil bottles with code No. 2., toys, and some plastic bags. PET (Polyethylene Terephthalate) PETE or PET is one of the plastics used for food containers, bottles of mineral water and several other wrappers. This plastic is designed for one-time use only. With the use of HDPE and PET plastic waste at a percentage of 20% for concrete compressive strength was not achieved, normal concrete = 15.88 concrete B.HDPE = 12.01, B.PET = 11.71, BC = 12.39 but for concrete weight decreasing, normal concrete = 2330 kg, m3 B.HDPE concrete = 2122 kg, m3, B.PET = 2128 kg, m3, BC = 2096 kg, m3. For the composition of the optimum concrete mixture of the three compositions (B.HDPE, B.PET, BC) obtained the composition of BC which has the most optimum value of 12.39 Mpa, but does not reach the compressive strength of the plan of 15 Mpa.\",\"PeriodicalId\":17796,\"journal\":{\"name\":\"JURNAL ILMIAH BERING'S\",\"volume\":\"2 1\",\"pages\":\"\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2019-10-07\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"JURNAL ILMIAH BERING'S\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.36050/berings.v6i02.194\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"JURNAL ILMIAH BERING'S","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.36050/berings.v6i02.194","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

一般来说,混凝土是由水泥、细骨料、粗骨料、水和必要的附加物质组成的。但随着科学技术的发展,混凝土成分材料也可以发生变化或与塑料废料等有机或无机材料相结合。HDPE塑料(高密度聚乙烯)是一种塑料,通常用于制造牛奶瓶,洗涤剂瓶,洗发水瓶,保湿瓶,油瓶,代码为2。玩具和一些塑料袋。PET(聚对苯二甲酸乙二醇酯)是一种用于食品容器、瓶装矿泉水和其他几种包装的塑料。这种塑料只能一次性使用。在HDPE和PET塑料废料用量为20%的情况下,混凝土抗压强度未达到,普通混凝土= 15.88,B.HDPE = 12.01, B.PET = 11.71, BC = 12.39,但混凝土自重降低,普通混凝土= 2330 kg, m3, B.HDPE混凝土= 2122 kg, m3, B.PET = 2128 kg, m3, BC = 2096 kg, m3。对于三种组合物(B.HDPE、B.PET、BC)的最佳混凝土配合比,得到了组合物BC的最优值为12.39 Mpa,但抗压强度未达到方案的15 Mpa。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
ANALISA PENGARUH SUBSTITUSI LIMBAH PLASTIK SEBAGAI AGREGAT KASAR TERHADAP KUAT TEKAN BETON
In general, concrete is composed of cement, fine aggregate, coarse aggregate, water and additional substances if needed. But along with the development of science and technology, concrete constituent materials can also change or be combined with organic or inorganic materials such as plastic waste materials and others. HDPE Plastic (High-Density Polyethylene) Is a type of plastic that is usually used to make milk bottles, detergent bottles, shampoo bottles, moisturizing bottles, oil bottles with code No. 2., toys, and some plastic bags. PET (Polyethylene Terephthalate) PETE or PET is one of the plastics used for food containers, bottles of mineral water and several other wrappers. This plastic is designed for one-time use only. With the use of HDPE and PET plastic waste at a percentage of 20% for concrete compressive strength was not achieved, normal concrete = 15.88 concrete B.HDPE = 12.01, B.PET = 11.71, BC = 12.39 but for concrete weight decreasing, normal concrete = 2330 kg, m3 B.HDPE concrete = 2122 kg, m3, B.PET = 2128 kg, m3, BC = 2096 kg, m3. For the composition of the optimum concrete mixture of the three compositions (B.HDPE, B.PET, BC) obtained the composition of BC which has the most optimum value of 12.39 Mpa, but does not reach the compressive strength of the plan of 15 Mpa.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信