{"title":"干燥O2对硅表面电导率的影响","authors":"N. G. Einspruch","doi":"10.1002/PSSB.19620020207","DOIUrl":null,"url":null,"abstract":"In order to evaluate the effects of dried oxygen on the electrical transport properties of the silicon surface, ac field effect measurements on a CP-4 etched surface have been made. The equilibrium surface potential of a sample stored in room air undergoes a 12 mv p-type shift upon exposure to dried O2. The field effect mobility changes from 0.11 (n-type) to 0.19 (p-type) cm2/volt sec. After the sample is exposed to dried O2, the applied electric field produces a total variation of the charge trapped in the surface states of 22mμ coul/cm2 with a corresponding variation in surface potential of 0.75 (e φ/k T units). \n \n \n \nUm den Einflus von getrocknetem Sauerstoff auf die elektrischen Transporteigenschaften der Siliziumoberflache zu untersuchen, wurden Wechselstrom-Feldeffektmessungen an einer mit CP-4 geatzten Oberflache ausgefuhrt. Das Gleichgewichts-Oberflachenpotential einer in Zimmerluft aufbewahrten Probe wird unter Einwirkung von getrocknetem O2 um 12 mV in p-Richtung verschoben. Die Feldeffekt-Beweglichkeit andert sich von 0,11 (n-Typ) bis 0,19 (p-Typ) cm2/V sec. Nachdem die Probe getrocknetem Sauerstoff ausgesetzt wurde, erzeugt das elektrische Feld eine Gesamtanderung der in den Oberflachenzustanden angehafteten Ladung von 22 mμ Coul/cm2, wobei sich das Oberflachenpotential um 0,75 kT/e andert.","PeriodicalId":74075,"journal":{"name":"Life sciences (1962)","volume":"625 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"1962-12-31","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"4","resultStr":"{\"title\":\"The Effects of Dried O2 on the Surface Conductance of Silicon\",\"authors\":\"N. G. Einspruch\",\"doi\":\"10.1002/PSSB.19620020207\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"In order to evaluate the effects of dried oxygen on the electrical transport properties of the silicon surface, ac field effect measurements on a CP-4 etched surface have been made. The equilibrium surface potential of a sample stored in room air undergoes a 12 mv p-type shift upon exposure to dried O2. The field effect mobility changes from 0.11 (n-type) to 0.19 (p-type) cm2/volt sec. After the sample is exposed to dried O2, the applied electric field produces a total variation of the charge trapped in the surface states of 22mμ coul/cm2 with a corresponding variation in surface potential of 0.75 (e φ/k T units). \\n \\n \\n \\nUm den Einflus von getrocknetem Sauerstoff auf die elektrischen Transporteigenschaften der Siliziumoberflache zu untersuchen, wurden Wechselstrom-Feldeffektmessungen an einer mit CP-4 geatzten Oberflache ausgefuhrt. Das Gleichgewichts-Oberflachenpotential einer in Zimmerluft aufbewahrten Probe wird unter Einwirkung von getrocknetem O2 um 12 mV in p-Richtung verschoben. Die Feldeffekt-Beweglichkeit andert sich von 0,11 (n-Typ) bis 0,19 (p-Typ) cm2/V sec. Nachdem die Probe getrocknetem Sauerstoff ausgesetzt wurde, erzeugt das elektrische Feld eine Gesamtanderung der in den Oberflachenzustanden angehafteten Ladung von 22 mμ Coul/cm2, wobei sich das Oberflachenpotential um 0,75 kT/e andert.\",\"PeriodicalId\":74075,\"journal\":{\"name\":\"Life sciences (1962)\",\"volume\":\"625 1\",\"pages\":\"\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"1962-12-31\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"4\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Life sciences (1962)\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1002/PSSB.19620020207\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Life sciences (1962)","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1002/PSSB.19620020207","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 4

摘要

为了评价干燥氧对硅表面电输运性质的影响,在CP-4蚀刻表面进行了交流场效应测量。储存在室内空气中的样品在暴露于干燥的O2时,其平衡表面电位发生12mv的p型位移。电场效应迁移率从0.11 (n型)变化到0.19 (p型)cm2/伏特秒。样品暴露于干燥的O2后,外加电场产生表面态捕获电荷的总变化为22μ coul/cm2,相应的表面电位变化为0.75 (e φ/k T单位)。研究发现:1 .研究发现:1 .发现:1 .发现:1 .发现:1 .发现:1 .发现:1 .发现:1 .发现:1 .发现:1 .发现:1 .发现:1 .发现:1 .发现:在p-Richtung verschoben中,在Einwirkung von getrocknetem O2和12mv下的探针风。Die Feldeffekt-Beweglichkeit andert sich von 0,11 (n-Typ)和0,19 (p-Typ) cm2/V秒。Nachdem Die Probe getrocknetem Sauerstoff ausgesetzt wurde, erzeugt das elektrische Feld eine Gesamtanderung der in den Oberflachenzustanden angehafteten Ladung von 22 μ Coul/cm2,其中bebesidas Oberflachenpotential um 0,75 kT/e andert。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
The Effects of Dried O2 on the Surface Conductance of Silicon
In order to evaluate the effects of dried oxygen on the electrical transport properties of the silicon surface, ac field effect measurements on a CP-4 etched surface have been made. The equilibrium surface potential of a sample stored in room air undergoes a 12 mv p-type shift upon exposure to dried O2. The field effect mobility changes from 0.11 (n-type) to 0.19 (p-type) cm2/volt sec. After the sample is exposed to dried O2, the applied electric field produces a total variation of the charge trapped in the surface states of 22mμ coul/cm2 with a corresponding variation in surface potential of 0.75 (e φ/k T units). Um den Einflus von getrocknetem Sauerstoff auf die elektrischen Transporteigenschaften der Siliziumoberflache zu untersuchen, wurden Wechselstrom-Feldeffektmessungen an einer mit CP-4 geatzten Oberflache ausgefuhrt. Das Gleichgewichts-Oberflachenpotential einer in Zimmerluft aufbewahrten Probe wird unter Einwirkung von getrocknetem O2 um 12 mV in p-Richtung verschoben. Die Feldeffekt-Beweglichkeit andert sich von 0,11 (n-Typ) bis 0,19 (p-Typ) cm2/V sec. Nachdem die Probe getrocknetem Sauerstoff ausgesetzt wurde, erzeugt das elektrische Feld eine Gesamtanderung der in den Oberflachenzustanden angehafteten Ladung von 22 mμ Coul/cm2, wobei sich das Oberflachenpotential um 0,75 kT/e andert.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信