{"title":"近地轨道太阳能发电机的黄金互连器","authors":"G. La Roche, C. Oxynos-Lauschke, K. Wehner","doi":"10.1109/WCPEC.1994.521659","DOIUrl":null,"url":null,"abstract":"For low Earth orbit applications gold based electrical connections have keen developed consisting of 12.5 /spl mu/m thin gold solar cell interconnectors with stress relief loop, 50 /spl mu/m thick gold string terminations and gauge AWG 24 stranded gold wires. Modules with typical 4 cm by 6 cm silicon solar cells mounted on a lightweight carbon fibre reinforced honeycomb substrate were manufactured including the new components applied by resistance welding. A long duration thermal cycling test was started cycling two coupons at between -110/spl deg/C and +110/spl deg/C. As of November 1994, 27500 cycles have been completed, and the test is continuing. Evaluation of module integrity at periodic intervals yielded no measurable degradation up to date.","PeriodicalId":20517,"journal":{"name":"Proceedings of 1994 IEEE 1st World Conference on Photovoltaic Energy Conversion - WCPEC (A Joint Conference of PVSC, PVSEC and PSEC)","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"1994-12-05","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Gold interconnectors for solar generators in low Earth orbits\",\"authors\":\"G. La Roche, C. Oxynos-Lauschke, K. Wehner\",\"doi\":\"10.1109/WCPEC.1994.521659\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"For low Earth orbit applications gold based electrical connections have keen developed consisting of 12.5 /spl mu/m thin gold solar cell interconnectors with stress relief loop, 50 /spl mu/m thick gold string terminations and gauge AWG 24 stranded gold wires. Modules with typical 4 cm by 6 cm silicon solar cells mounted on a lightweight carbon fibre reinforced honeycomb substrate were manufactured including the new components applied by resistance welding. A long duration thermal cycling test was started cycling two coupons at between -110/spl deg/C and +110/spl deg/C. As of November 1994, 27500 cycles have been completed, and the test is continuing. Evaluation of module integrity at periodic intervals yielded no measurable degradation up to date.\",\"PeriodicalId\":20517,\"journal\":{\"name\":\"Proceedings of 1994 IEEE 1st World Conference on Photovoltaic Energy Conversion - WCPEC (A Joint Conference of PVSC, PVSEC and PSEC)\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":0.0000,\"publicationDate\":\"1994-12-05\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Proceedings of 1994 IEEE 1st World Conference on Photovoltaic Energy Conversion - WCPEC (A Joint Conference of PVSC, PVSEC and PSEC)\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1109/WCPEC.1994.521659\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Proceedings of 1994 IEEE 1st World Conference on Photovoltaic Energy Conversion - WCPEC (A Joint Conference of PVSC, PVSEC and PSEC)","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1109/WCPEC.1994.521659","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
Gold interconnectors for solar generators in low Earth orbits
For low Earth orbit applications gold based electrical connections have keen developed consisting of 12.5 /spl mu/m thin gold solar cell interconnectors with stress relief loop, 50 /spl mu/m thick gold string terminations and gauge AWG 24 stranded gold wires. Modules with typical 4 cm by 6 cm silicon solar cells mounted on a lightweight carbon fibre reinforced honeycomb substrate were manufactured including the new components applied by resistance welding. A long duration thermal cycling test was started cycling two coupons at between -110/spl deg/C and +110/spl deg/C. As of November 1994, 27500 cycles have been completed, and the test is continuing. Evaluation of module integrity at periodic intervals yielded no measurable degradation up to date.