Betul Busra Ursavas, T. Bezgin, Mert Ocak, B. Bilecenoğlu, Ayşe Işıl Orhan
{"title":"不同蚀刻方式通用胶粘剂在复合材料修复体中微渗漏的体外评价","authors":"Betul Busra Ursavas, T. Bezgin, Mert Ocak, B. Bilecenoğlu, Ayşe Işıl Orhan","doi":"10.5114/jos.2021.111657","DOIUrl":null,"url":null,"abstract":"Introduction: In order to obtain a good prognosis in resin restorations, a strong adhesion not allowing leakage between tooth tissues and restoration should be provided. Effectiveness of universal adhesives on leakage in primary teeth compomer restorations has not been studied. Objectives: The objective of this study was to evaluate sealing ability of a universal adhesive used with different etching modes after 1- and 3-year of artificial aging in compomer restorations of primary teeth. Material and methods: Sixty-three extracted mandibular primary second molars were used in the study. Class II box cavities (3 mm × 3 mm × 1.5 mm) were prepared in each tooth. Then, teeth were divided into three groups ( n = 21), including total-etch, self-etch, and selective-etch modes. All teeth were restored with compomer (Dyract Extra, Dentsply; Konstanz, Germany) after universal adhesive (Prime & Bond Elect Universal, Denstsply; Milford, USA) application. Teeth were divided into three sub-groups ( n = 7) with the following three different aging protocols: 24 h water storage, 1-year aging, and 3-year aging with chewing simulator (Esetron Chewing Simulator; Ankara, Turkey). 50% silver nitrate solution was applied as a tracer, and its’ penetration was analyzed in mm3 using micro-computed tomography system (SkyScan 1275; Kontich, Belgium). Data was analyzed with Kruskal-Wallis H and Friedman tests. Results: One-year aging significantly increased the leakage in self-etch group of samples (0.197 ± 0.49 mm 3 ) compared to the total-etch (0.001 ± 0.000 mm 3 ) and selective-etch (0.001 ± 0.000 mm 3 ) groups ( p < 0.05). There was no diffe rence between the groups at baseline and after the 3-year artificial aging ( p > 0.05). Conclusions: Self-etch mode of adhesive revealed higher micro-leakage levels at all examination intervals; how-ever, the difference was only significant after the 1-year aging. It can be concluded that universal adhesives can be used with all etching modes in compomer restorations.","PeriodicalId":35469,"journal":{"name":"Journal of Stomatology","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"2021-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"In-vitro evaluation of micro-leakage of a universal adhesive used with different etching modes in compomer restorations\",\"authors\":\"Betul Busra Ursavas, T. Bezgin, Mert Ocak, B. Bilecenoğlu, Ayşe Işıl Orhan\",\"doi\":\"10.5114/jos.2021.111657\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Introduction: In order to obtain a good prognosis in resin restorations, a strong adhesion not allowing leakage between tooth tissues and restoration should be provided. Effectiveness of universal adhesives on leakage in primary teeth compomer restorations has not been studied. Objectives: The objective of this study was to evaluate sealing ability of a universal adhesive used with different etching modes after 1- and 3-year of artificial aging in compomer restorations of primary teeth. Material and methods: Sixty-three extracted mandibular primary second molars were used in the study. Class II box cavities (3 mm × 3 mm × 1.5 mm) were prepared in each tooth. Then, teeth were divided into three groups ( n = 21), including total-etch, self-etch, and selective-etch modes. All teeth were restored with compomer (Dyract Extra, Dentsply; Konstanz, Germany) after universal adhesive (Prime & Bond Elect Universal, Denstsply; Milford, USA) application. Teeth were divided into three sub-groups ( n = 7) with the following three different aging protocols: 24 h water storage, 1-year aging, and 3-year aging with chewing simulator (Esetron Chewing Simulator; Ankara, Turkey). 50% silver nitrate solution was applied as a tracer, and its’ penetration was analyzed in mm3 using micro-computed tomography system (SkyScan 1275; Kontich, Belgium). Data was analyzed with Kruskal-Wallis H and Friedman tests. Results: One-year aging significantly increased the leakage in self-etch group of samples (0.197 ± 0.49 mm 3 ) compared to the total-etch (0.001 ± 0.000 mm 3 ) and selective-etch (0.001 ± 0.000 mm 3 ) groups ( p < 0.05). There was no diffe rence between the groups at baseline and after the 3-year artificial aging ( p > 0.05). Conclusions: Self-etch mode of adhesive revealed higher micro-leakage levels at all examination intervals; how-ever, the difference was only significant after the 1-year aging. It can be concluded that universal adhesives can be used with all etching modes in compomer restorations.\",\"PeriodicalId\":35469,\"journal\":{\"name\":\"Journal of Stomatology\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2021-01-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Journal of Stomatology\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.5114/jos.2021.111657\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q4\",\"JCRName\":\"Dentistry\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Stomatology","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.5114/jos.2021.111657","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"Dentistry","Score":null,"Total":0}
引用次数: 0
摘要
在树脂修复体中,为了获得良好的预后,需要在牙组织与修复体之间提供不渗漏的强附着力。通用粘接剂治疗乳牙复合修复体渗漏的效果尚未见研究。目的:本研究的目的是评估一种通用胶粘剂在人工老化1年和3年后不同蚀刻模式下对乳牙复合修复体的密封能力。材料与方法:采用63颗拔除的下颌初级第二磨牙进行研究。在每颗牙齿上制备3 mm × 3 mm × 1.5 mm的II类箱形腔。然后,将牙齿分为三组(n = 21),包括全蚀、自蚀和选择性蚀模式。所有牙齿均使用comomer (Dyract Extra, Dentsply;康斯坦茨,德国)万能胶(Prime & Bond Elect universal, Denstsply;Milford, USA)申请。将牙齿分为3个亚组(n = 7),采用以下3种不同的老化方案:24 h水储存,1年老化,3年老化使用咀嚼模拟器(Esetron咀嚼模拟器;安卡拉,土耳其)。用50%硝酸银溶液作为示踪剂,用微计算机断层扫描系统(SkyScan 1275;Kontich、比利时)。数据分析采用Kruskal-Wallis H和Friedman检验。结果:与全蚀组(0.001±0.000 mm 3)和选择性蚀组(0.001±0.000 mm 3)相比,自蚀组(0.197±0.49 mm 3)老化1年显著增加(p < 0.05)。人工衰老3年后各组间差异无统计学意义(p < 0.05)。结论:自蚀刻方式的胶粘剂在各检测间隔均显示出较高的微渗漏水平;然而,只有在1年后,这种差异才显着。结果表明,通用胶粘剂可用于各种蚀刻方式的复合材料修复。
In-vitro evaluation of micro-leakage of a universal adhesive used with different etching modes in compomer restorations
Introduction: In order to obtain a good prognosis in resin restorations, a strong adhesion not allowing leakage between tooth tissues and restoration should be provided. Effectiveness of universal adhesives on leakage in primary teeth compomer restorations has not been studied. Objectives: The objective of this study was to evaluate sealing ability of a universal adhesive used with different etching modes after 1- and 3-year of artificial aging in compomer restorations of primary teeth. Material and methods: Sixty-three extracted mandibular primary second molars were used in the study. Class II box cavities (3 mm × 3 mm × 1.5 mm) were prepared in each tooth. Then, teeth were divided into three groups ( n = 21), including total-etch, self-etch, and selective-etch modes. All teeth were restored with compomer (Dyract Extra, Dentsply; Konstanz, Germany) after universal adhesive (Prime & Bond Elect Universal, Denstsply; Milford, USA) application. Teeth were divided into three sub-groups ( n = 7) with the following three different aging protocols: 24 h water storage, 1-year aging, and 3-year aging with chewing simulator (Esetron Chewing Simulator; Ankara, Turkey). 50% silver nitrate solution was applied as a tracer, and its’ penetration was analyzed in mm3 using micro-computed tomography system (SkyScan 1275; Kontich, Belgium). Data was analyzed with Kruskal-Wallis H and Friedman tests. Results: One-year aging significantly increased the leakage in self-etch group of samples (0.197 ± 0.49 mm 3 ) compared to the total-etch (0.001 ± 0.000 mm 3 ) and selective-etch (0.001 ± 0.000 mm 3 ) groups ( p < 0.05). There was no diffe rence between the groups at baseline and after the 3-year artificial aging ( p > 0.05). Conclusions: Self-etch mode of adhesive revealed higher micro-leakage levels at all examination intervals; how-ever, the difference was only significant after the 1-year aging. It can be concluded that universal adhesives can be used with all etching modes in compomer restorations.