具有细丝和Cu稳定化的YBCO导体的交流损耗(50- 200hz)

M. Sumption, A. Contractor, S. Kawabata, E. Collings
{"title":"具有细丝和Cu稳定化的YBCO导体的交流损耗(50- 200hz)","authors":"M. Sumption, A. Contractor, S. Kawabata, E. Collings","doi":"10.1063/1.2192437","DOIUrl":null,"url":null,"abstract":"AC loss measurements have been made on YBCO coated conductors in externally applied sinusoidal AC fields using the pick‐up coil method. Various arrangements of YBCO coated conductor have been measured at frequencies of 50 Hz, 75 Hz, 100 Hz, 150 Hz, and 200 Hz, with amplitudes ranging from 0 to 140 mT. Three different sets of IBAD‐based YBCO coated conductor were measured: (i) unfilamented conductors with Cu added either on one side only, or on both sides (as well as the edges), (ii) conductors with various numbers of filament, (iii) 4 mm wide conductors. All samples were 4 cm long and untwisted. The per cycle AC loss per unit length of conductor, displayed in the format Q/B (in J/T.m) vs. Bm. enabled separation of the eddy current and hysteretic components of the total loss, after which the results were analyzed and discussed. The resistivity of the interfilamentary connections were characterized and the results compared to expectation.","PeriodicalId":80359,"journal":{"name":"Advances in cryogenic engineering","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"2006-04-21","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://sci-hub-pdf.com/10.1063/1.2192437","citationCount":"1","resultStr":"{\"title\":\"AC loss (50-200 Hz) in YBCO conductors with filaments and Cu stabilization\",\"authors\":\"M. Sumption, A. Contractor, S. Kawabata, E. Collings\",\"doi\":\"10.1063/1.2192437\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"AC loss measurements have been made on YBCO coated conductors in externally applied sinusoidal AC fields using the pick‐up coil method. Various arrangements of YBCO coated conductor have been measured at frequencies of 50 Hz, 75 Hz, 100 Hz, 150 Hz, and 200 Hz, with amplitudes ranging from 0 to 140 mT. Three different sets of IBAD‐based YBCO coated conductor were measured: (i) unfilamented conductors with Cu added either on one side only, or on both sides (as well as the edges), (ii) conductors with various numbers of filament, (iii) 4 mm wide conductors. All samples were 4 cm long and untwisted. The per cycle AC loss per unit length of conductor, displayed in the format Q/B (in J/T.m) vs. Bm. enabled separation of the eddy current and hysteretic components of the total loss, after which the results were analyzed and discussed. The resistivity of the interfilamentary connections were characterized and the results compared to expectation.\",\"PeriodicalId\":80359,\"journal\":{\"name\":\"Advances in cryogenic engineering\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2006-04-21\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"https://sci-hub-pdf.com/10.1063/1.2192437\",\"citationCount\":\"1\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Advances in cryogenic engineering\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1063/1.2192437\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Advances in cryogenic engineering","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1063/1.2192437","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 1

摘要

在外部正弦交流磁场中,用检波线圈法测量了YBCO涂层导体的交流损耗。在50hz, 75hz, 100hz, 150hz和200hz的频率范围内,测量了不同排列的YBCO涂层导体,幅度从0到140 mT。测量了三种不同的IBAD基YBCO涂层导体:(i)仅在一侧或两侧(以及边缘)添加Cu的无丝导体,(ii)具有不同数量的丝的导体,(iii) 4mm宽的导体。所有的样品都是4厘米长,没有扭曲。单位长度导体的每周期交流损耗,以Q/B (J/T.m) vs. Bm的格式显示。使总损耗的涡流和滞后分量分离,然后对结果进行分析和讨论。对纤维间连接的电阻率进行了表征,并与预期结果进行了比较。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
AC loss (50-200 Hz) in YBCO conductors with filaments and Cu stabilization
AC loss measurements have been made on YBCO coated conductors in externally applied sinusoidal AC fields using the pick‐up coil method. Various arrangements of YBCO coated conductor have been measured at frequencies of 50 Hz, 75 Hz, 100 Hz, 150 Hz, and 200 Hz, with amplitudes ranging from 0 to 140 mT. Three different sets of IBAD‐based YBCO coated conductor were measured: (i) unfilamented conductors with Cu added either on one side only, or on both sides (as well as the edges), (ii) conductors with various numbers of filament, (iii) 4 mm wide conductors. All samples were 4 cm long and untwisted. The per cycle AC loss per unit length of conductor, displayed in the format Q/B (in J/T.m) vs. Bm. enabled separation of the eddy current and hysteretic components of the total loss, after which the results were analyzed and discussed. The resistivity of the interfilamentary connections were characterized and the results compared to expectation.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信