{"title":"FeAl金属间相基体合金在600℃、700℃和800℃氧化后的表面状态","authors":"J. Cebulski","doi":"10.15199/40.2023.4.1","DOIUrl":null,"url":null,"abstract":"","PeriodicalId":42782,"journal":{"name":"Ochrona Przed Korozja","volume":" ","pages":""},"PeriodicalIF":0.2000,"publicationDate":"2023-04-21","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Surface state of alloy based on FeAl intermetallic phase matrix after oxidation at 600°C, 700°C and 800°C\",\"authors\":\"J. Cebulski\",\"doi\":\"10.15199/40.2023.4.1\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"\",\"PeriodicalId\":42782,\"journal\":{\"name\":\"Ochrona Przed Korozja\",\"volume\":\" \",\"pages\":\"\"},\"PeriodicalIF\":0.2000,\"publicationDate\":\"2023-04-21\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Ochrona Przed Korozja\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.15199/40.2023.4.1\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q4\",\"JCRName\":\"MATERIALS SCIENCE, MULTIDISCIPLINARY\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Ochrona Przed Korozja","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.15199/40.2023.4.1","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"MATERIALS SCIENCE, MULTIDISCIPLINARY","Score":null,"Total":0}