M. Monsalve-Arias, Ó. Higuera-Cobos, H. Ageorges, F. Vargas-Galvis, M. López-Gómez
{"title":"热喷涂生物活性玻璃涂层的磨损行为","authors":"M. Monsalve-Arias, Ó. Higuera-Cobos, H. Ageorges, F. Vargas-Galvis, M. López-Gómez","doi":"10.19053/01211129.v31.n62.2022.14778","DOIUrl":null,"url":null,"abstract":"In this work, bioactive glass coatings were fabricated by plasma thermal spraying and oxyacetylene flame techniques from 2 different bioactive glass powders with 0 and 2% molar MgO. The metal substrates used were Ti6Al4V alloy and AISI 316L steel. The tribological behavior of the coatings was evaluated by the ball-on-disc method in the presence of simulated biological fluid (SBF), and the results were correlated with their mechanical behavior, obtaining values of hardness (between 4.84 and 5.18 GPa) and fracture toughness (between 5.25 and 6.62 MPa.m1/2). The results show that fracture toughness has a slightly higher effect than hardness on the wear behavior of the coatings under study.","PeriodicalId":42846,"journal":{"name":"Revista Facultad de Ingenieria, Universidad Pedagogica y Tecnologica de Colombia","volume":null,"pages":null},"PeriodicalIF":0.2000,"publicationDate":"2022-11-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Wear Behavior of Bioactive Glass Coatings Deposited by Thermal Spraying\",\"authors\":\"M. Monsalve-Arias, Ó. Higuera-Cobos, H. Ageorges, F. Vargas-Galvis, M. López-Gómez\",\"doi\":\"10.19053/01211129.v31.n62.2022.14778\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"In this work, bioactive glass coatings were fabricated by plasma thermal spraying and oxyacetylene flame techniques from 2 different bioactive glass powders with 0 and 2% molar MgO. The metal substrates used were Ti6Al4V alloy and AISI 316L steel. The tribological behavior of the coatings was evaluated by the ball-on-disc method in the presence of simulated biological fluid (SBF), and the results were correlated with their mechanical behavior, obtaining values of hardness (between 4.84 and 5.18 GPa) and fracture toughness (between 5.25 and 6.62 MPa.m1/2). The results show that fracture toughness has a slightly higher effect than hardness on the wear behavior of the coatings under study.\",\"PeriodicalId\":42846,\"journal\":{\"name\":\"Revista Facultad de Ingenieria, Universidad Pedagogica y Tecnologica de Colombia\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":0.2000,\"publicationDate\":\"2022-11-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Revista Facultad de Ingenieria, Universidad Pedagogica y Tecnologica de Colombia\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.19053/01211129.v31.n62.2022.14778\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q4\",\"JCRName\":\"ENGINEERING, MULTIDISCIPLINARY\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Revista Facultad de Ingenieria, Universidad Pedagogica y Tecnologica de Colombia","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.19053/01211129.v31.n62.2022.14778","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"ENGINEERING, MULTIDISCIPLINARY","Score":null,"Total":0}
引用次数: 0

摘要

本文采用等离子体热喷涂和氧乙炔火焰技术,将两种不同的生物活性玻璃粉分别添加0和2%摩尔氧化镁,制备了生物活性玻璃涂层。金属基体为Ti6Al4V合金和AISI 316L钢。在模拟生物流体(SBF)存在的情况下,采用球盘法对涂层的摩擦学行为进行了评估,结果与涂层的力学行为相关联,获得了硬度(4.84 ~ 5.18 GPa)和断裂韧性(5.25 ~ 6.62 mpa . m2 /2)的值。结果表明,断裂韧性对涂层磨损性能的影响略高于硬度。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
Wear Behavior of Bioactive Glass Coatings Deposited by Thermal Spraying
In this work, bioactive glass coatings were fabricated by plasma thermal spraying and oxyacetylene flame techniques from 2 different bioactive glass powders with 0 and 2% molar MgO. The metal substrates used were Ti6Al4V alloy and AISI 316L steel. The tribological behavior of the coatings was evaluated by the ball-on-disc method in the presence of simulated biological fluid (SBF), and the results were correlated with their mechanical behavior, obtaining values of hardness (between 4.84 and 5.18 GPa) and fracture toughness (between 5.25 and 6.62 MPa.m1/2). The results show that fracture toughness has a slightly higher effect than hardness on the wear behavior of the coatings under study.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
审稿时长
8 weeks
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信